Polymer Property : Melting Point = 1816 °C Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Melting Point 1816 °C
3301 °F
Unifrax Fiberfrax® Duraboard® 2600 Ceramic Fiber Board
Fiberfrax® Duraboard® products are a family of rigid, high-temperature ceramic fiber boards manufactured in a wet forming process using Fiberfrax alumina-silica fibers and binders. All Duraboard ..