Material Notes:
Description: UBE Super Polyethylene Umerit® is an ethylene-olefin copolymer made by UBE using the metallocene catalytic method. The metallocene catalytic method results in superior physical properties by being able to acquire any targeted molecular structures. Specific Notes for this Grade: UMERIT® 500F offers various excellent properties: Superior low temperature seal property, advantageous compared to 1500F, Reduced motor load at processing, Draw resonance at high-speed drawing hardly occurs.Information provided by UBE.
Physical Properties Metric English Comments
Density 0.904 g/cc
0.0327 lb/in³
ASTM D1505
Environmental Stress Crack Resistance 1000 hour
1000 hour
F50; ASTM D1693
Melt Flow 4.0 g/10 min
4.0 g/10 min
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Shore D 44
44
ASTM D2240
Tensile Strength, Yield 42.0 MPa
6090 psi
ASTM D638
Elongation at Break 715 %
715 %
ASTM D638
Tensile Modulus 0.140 GPa
20.3 ksi
Bending Modulus; ASTM D790
Thermal Properties Metric English Comments
Melting Point 87.0 °C
189 °F
UBE method
Vicat Softening Point 81.0 °C
178 °F
ASTM D1525