Thermal Properties | Metric | English | Comments |
---|---|---|---|
Melting Point | 87.2 °C | 189 °F | Peak Melting Temperature; ExxonMobil Method |
ExxonMobil ESCOR™ AT 310 Cast Film Resin
(discontinued **) ESCOR AT 310 is an acid terpolymer which provides excellent adhesion to a variety of polar and non-polar materials such as metals, glass, polyolefins, polyamides, polyesters, etc. It is suitable fo.. |
|||
Melting Point | 87.0 °C | 189 °F | DSC; ASTM D3418 |
DuPont Bynel® 39E622 Adhesive Resin
(discontinued **) Bynel® Series 3900 resins are anhydride-modified ethylene vinyl acetate polymers. They are available in pellet form for use in conventional extrusion and coextrusion equipment designed to process p.. |
|||
Melting Point | 87.0 °C | 189 °F | Melting point via DSC/ASTM D3418 |
DuPont Bynel® E326 Acid-/Acrylate-Modified EVA Adhesive Resin
(discontinued **) Bynel® Series 3100 resins are acid/acrylate-modified ethylene vinyl acetate polymers. They are available in pellet form for use in conventional extrusion and coextrusion equipment designed to proce.. |
|||
Melting Point | 87.0 °C | 189 °F | Upon Melting via DSC/ASTM D3418 |
DuPont Elvax® 3174SHB Ethylene-Vinyl Acetate Copolymer Resin for Coextrusion, Cast Film
(discontinued **) 18 wt% Vinyl Acetate.General Elvax® information: Elvax® packaging grade resins include low seal temperatures for use in coextrusions or for packaging temperature sensitive materials, excellent dra.. |
|||
Melting Point | 87.2 °C | 189 °F | Peak Melting Temperature; ExxonMobil Method |
ExxonMobil Escorene® LD 725.21 Molding, extrusion, compounding and adhesive resin
(discontinued **) Escorene Ultra LD 722.21 is 18 wt% vinyl acetate copolymer suitable for molding, extrusion, compounding and hot melt adhesive applications.Information provided by ExxonMobil Chemical |
|||
Melting Point | 87.0 - 93.0 °C | 189 - 199 °F | |
Indium Corp. Indalloy 36 Bismuth Solder Alloy Information Provided by Indium Corporation |
|||
Melting Point | 87.0 - 91.0 °C | 189 - 196 °F | |
Indium Corp. Indalloy 33 Bismuth Solder Alloy Information Provided by Indium Corporation |
|||
Melting Point | 87.0 °C | 189 °F | Freezing Point, DSC; ASTM D3418 |
DuPont Bynel® 30E671 Adhesive Resin Bynel® Series 3000 resins are anhydride-modified ethylene vinyl acetate polymers. They are available in pellet form for use in conventional extrusion and coextrusion equipment designed to process p.. |
|||
Melting Point | 87.0 °C | 189 °F | DSC; ASTM D3418 |
DuPont Bynel® 3126 Adhesive Resin Bynel® Series 3100 resins are acid/acrylate-modified ethylene vinyl acetate polymers. They are available in pellet form for use in conventional extrusion and coextrusion equipment designed to proce.. |
|||
Melting Point | 87.0 °C | 189 °F | Upon Melting via DSC/ASTM D3418 |
DuPont Elvax® 3170 Ethylene-Vinyl Acetate Copolymer Resin for Coextrusion, Blown Film 18 wt% Vinyl Acetate.Elvax® 3170 is an extrudable ethylene-vinyl acetate copolymer resin available in pellet form for use in conventional extrusion equipment designed to process polyethylene resins.. |
|||
Melting Point | 87.0 °C | 189 °F | Upon Melting via DSC/ASTM D3418 |
DuPont Elvax® 3170SHB Ethylene-Vinyl Acetate Copolymer Resin for Coextrusion, Blown Film 18 wt% Vinyl Acetate.Elvax® 3170SHB is an extrudable ethylene-vinyl acetate copolymer resin available in pellet form for use in conventional extrusion equipment designed to process polyethylene res.. |
|||
Melting Point | 87.0 °C | 189 °F | Upon Melting via DSC/ASTM D3418 |
DuPont Elvax® 3176 Ethylene-Vinyl Acetate Copolymer Resin for Coextrusion, Extrusion Coating 18 wt% Vinyl Acetate.Elvax® 3176 is an extrudable ethylene-vinyl acetate copolymer resin available in pellet form for use in conventional extrusion equipment designed to process polyethylene resins.. |
|||
Melting Point | 87.0 °C | 189 °F | ISO 11357 |
Total EVA 1020 VN 5 Ethylene Vinyl Acetate Copolymer - Blown Film EVA 1020 VN 5 is made by a high pressure tubular process. Grade for very flexible films with very high transparency and good mechanical properties. Contains an antioxidant.Application examples: Ch.. |
|||
Melting Point | 87.0 °C | 189 °F | Melting point via DSC/ASTM D3418 |
DuPont Bynel® 2022 Acid-Modified Ethylene Terpolymer Adhesive Resin Bynel® Series 2000 resins are acid-modified ethylene terpolymers with medium to high acid comonomer contents. They contain a temperature stable ester that makes them functional in high-temperature .. |
|||
Melting Point | 87.0 °C | 189 °F | ASTM D3418, ISO 3146 |
DuPont™ Elvax® 3155 Ethylene Vinyl Acetate DuPont™ Elvax® 3155 is an extrudable ethylene-vinyl acetate copolymer resin available in pellet form for use in conventional extrusion equipment designed to process polyethylene resins. ELVAX® 31.. |
|||
Melting Point | 87.0 °C | 189 °F | DTA |
DuPont™ Surlyn® 9950 Ionomer Resin, Zinc Surlyn® 9950 thermoplastic resin is an advanced ethylene/methacrylic acid (E/MAA) copolymer, in which the MAA acid groups have been partially neutralized with zinc ions. The amount of MAA and neutr.. |
|||
Melting Point | 87.2 °C | 189 °F | Peak Melting Temperature; ExxonMobil Method |
ExxonMobil Escorene® LD 728.61 Molding, extrusion and compounding resin Escorene Ultra LD 728.61 is a high vinyl acetate copolymer with low melting temperature and excellent strength properties and toughness.Availability: Latin America, North America and South America A.. |
|||
Melting Point | 87.0 °C | 189 °F | Exxon Method |
ExxonMobil Iotek® 8030 Sodium Ionomer Molding/Extrusion Resin
(discontinued **) Data provided by the manufacturer, Exxon Chemical.Excellent abrasion resistance, impact strength, hardness, and tensile strength. Iotek ionomers provide superb low temperature impact strength when .. |
|||
Melting Point | 87.0 - 90.0 °C | 189 - 194 °F | |
BASF 2,5-Dimethyl-2,5-hexanediol Formula: C8H18O2CAS: 110-03-2Description: Dimethylhexanediol is a colorless to yellow solid, and is odorless. It is soluble in water and easily soluble in alcohols and acetone.Synonyms: 2,5-Dimethy.. |
|||
Melting Point | 87.0 °C | 189 °F | ASTM D3417 |
DuPont Elvax® 3550SBH Ethylene Vinyl Acetate
(discontinued **) DuPont™ Elvax® 3550SBH is an extrudable ethylene-vinyl acetate copolymer resin available in pellet form for use in conventional extrusion equipment designed to process polyethylene resins. Additiv.. |
|||
Melting Point | 87.0 °C | 189 °F | Upon Melting via DSC/ASTM D3418 |
DuPont Elvax® 3173SHB Ethylene-Vinyl Acetate Copolymer Resin for Coextrusion, Blown Film
(discontinued **)< 18 wt% Vinyl Acetate.Elvax® 3173SHB is an extrudable ethylene-vinyl acetate copolymer resin available in pellet form for use in conventional extrusion equipment designed to process polyethylene res.. |