Tra-Con Tra-Bond Ablebond 744-2NTN1 Electrically Insulating Polyimide Adhesive

Category Polymer , Adhesive , Thermoset , Epoxy
Manufacturer Tra-Con, Inc.
Trade Name Tra-Bond
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Tra-Con Tra-Bond Ablebond 744-2NTN1 Electrically Insulating Polyimide Adhesive.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Ablebond 744-2NTN1 structural epoxy adhesive is a nonsag version of 744-2 adhesive. Information provided by Tra-Con Inc.
Physical Properties Metric English Comments
Viscosity 24000 cP
24000 cP
Mixed
Mechanical Properties Metric English Comments
Hardness, Shore D 85
85
Adhesive Bond Strength 17.2 MPa
2500 psi
Lap shear, alum to alum
Processing Properties Metric English Comments
Cure Time 120 min

@Temperature 100 °C
2.00 hour

@Temperature 212 °F
240 min

@Temperature 75.0 °C
4.00 hour

@Temperature 167 °F
Shelf Life 12.0 Month

@Temperature -40.0 °C
12.0 Month

@Temperature -40.0 °F
Copyright © lookpolymers.com All Rights Reserved