BASF Palusol® 210 Silicate Panel

Category Other Engineering Material
Manufacturer BASF
Trade Name Palusol®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF BASF Palusol® 210 Silicate Panel.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Relevant identified uses: Intumescent plates for use as fire protection in the building industryInformation provided by BASF
Physical Properties Metric English Comments
Density 1.20 - 2.20 g/cc

@Pressure 0.101 MPa,
Temperature 20.0 °C
0.0434 - 0.0795 lb/in³

@Pressure 14.7 psi,
Temperature 68.0 °F
Solubility in Water 19.5 %
19.5 %
20°C, 1013hPa
pH 9.5
9.5
Thermal Properties Metric English Comments
Decomposition Temperature >= 100 °C
>= 212 °F
Descriptive Properties Value Comments
Color White
Commercial Status Europe