Material Notes:
TRA-BOND 7560D is an electrically insulating epoxy adhesive. This material has a 10 day work life and a medium viscosity for easy usage. There are also multiple cure options that make this product ideal for all electronic applications. TRA-BOND 7560D has excellent thermal conductivity.Information provided by Tra-Con Inc.
Physical Properties Metric English Comments
Viscosity 58000 cP

@Temperature 25.0 °C
58000 cP

@Temperature 77.0 °F
After mixing
Mechanical Properties Metric English Comments
Hardness, Shore D 87
87
Adhesive Bond Strength 16.5 MPa
2400 psi
Lap shear, alum to alum, @ 25°C
Thermal Properties Metric English Comments
CTE, linear 77.0 µm/m-°C
42.8 µin/in-°F
Below Tg
300 µm/m-°C
167 µin/in-°F
Above Tg
Thermal Conductivity 1.10 W/m-K

@Temperature 121 °C
7.63 BTU-in/hr-ft²-°F

@Temperature 250 °F
Glass Transition Temp, Tg 92.0 °C
198 °F
Ultimate Tg
Electrical Properties Metric English Comments
Volume Resistivity 1.50e+15 ohm-cm
1.50e+15 ohm-cm
Dielectric Constant 4.4
4.4
Dissipation Factor 0.0050

@Frequency 1000 Hz
0.0050

@Frequency 1000 Hz
Chemical Properties Metric English Comments
Ionic Impurities - Na (Sodium) 10 ppm
10 ppm
Ionic Impurities - K (Potassium) 0.00 ppm
0.00 ppm
Ionic Impurities - Cl (Chloride) 80 ppm
80 ppm
Processing Properties Metric English Comments
Cure Time 2.00 min

@Temperature 150 °C
0.0333 hour

@Temperature 302 °F
10.0 min

@Temperature 120 °C
0.167 hour

@Temperature 248 °F
Shelf Life 12.0 Month

@Temperature -40.0 °C
12.0 Month

@Temperature -40.0 °F
Descriptive Properties Value Comments
Working Life days 10