Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Adhesive Bond Strength | 16.5 MPa | 2400 psi | lap shear (on grit blasted steel, bond line thickness of 0.010"); ASTM D1002 |
ITW Devcon 10 minuteâ„¢ Epoxy, Black Information provided by ITW Devcon |
|||
Adhesive Bond Strength | 16.5 MPa | 2400 psi | lap shear (on grit blasted steel, bond line thickness of 0.010"); ASTM D1002 |
ITW Devcon 10 minuteâ„¢ Epoxy, Clear Information provided by ITW Devcon |
|||
Adhesive Bond Strength | >= 16.5 MPa | >= 2400 psi | shear, Al/Al, after 30 days water immersion |
Master Bond EP21TDCHT-LO Room Temperature Curing, Toughened Two Component Epoxy Master Bond Polymer Adhesive EP21TDCHT-LO is a two component epoxy adhesive formulated to cure at room temperature or more rapidly at elevated temperatures, with a very forgiving and convenient one .. |
|||
Adhesive Bond Strength | 16.5 MPa | 2400 psi | Lap shear, adhesion to glass |
Tra-Con Tra-Bond 2212 High Temperature Epoxy Adhesive TRA-BOND 2212 was developed for high temperature bonding, laminating, filament winding and potting applications where the combination of good physical and mechanical properties plus superior wetting.. |
|||
Adhesive Bond Strength | 16.5 MPa | 2400 psi | Lap shear, alum to alum, 1 hr @ 65°C |
Tra-Con Tra-Bond 716K02 Thixotropic Adhesive 716K02 is a more thixotropic version of FDA2T. Information provided by Tra-Con Inc. |
|||
Adhesive Bond Strength | 16.5 MPa | 2400 psi | Lap shear, alum to alum, @ 25°C |
Tra-Con Tra-Bond 7560D Hydrolytically Stable Adhesive TRA-BOND 7560D is an electrically insulating epoxy adhesive. This material has a 10 day work life and a medium viscosity for easy usage. There are also multiple cure options that make this product i.. |
|||
Adhesive Bond Strength | 16.5 MPa | 2400 psi | Lap shear, alum to alum |
Tra-Con Tra-Bond 77-1S One Component SMD Adhesive TRA-BOND 77-1S one component, solvent-free, insulating epoxy adhesive is designed specifically for attaching surface mounted devices (SMDs) to printed circuit boards prior to wave solder. TRA-BOND 7.. |
|||
Adhesive Bond Strength | 16.5 MPa | 2400 psi | Lap shear, alum to alum, 1 hr @ 65°C |
Tra-Con Tra-Bond FDA25 Food and Drug Application Epoxy Adhesive TRA-BOND FDA-25 is a medium viscosity epoxy resin system specifically developed for bonding and coating applications in accordance with Title 21, U.S. Code of Federal Regulations, Food and Drug Admi.. |
|||
Adhesive Bond Strength | 16.5 MPa | 2400 psi | |
Trelleborg Emerson & Cuming Eccobond® 45C Two-Component General Purpose Epoxy Adhesive Emerson & Cuming 45C Eccobond® Two-Component General Purpose Epoxy AdhesiveClear, unfilled, general purpose, room temperature curing, epoxy adhesive and sealant. Flexibility can be adjusted by the .. |
|||
Adhesive Bond Strength | 16.5 MPa | 2400 psi | |
Trelleborg Emerson & Cuming Eccobond® 45LV Two-Component General Purpose Epoxy Adhesive Emerson & Cuming 45LV Eccobond® Two-Component General Purpose Epoxy AdhesiveLow viscosity, filled, general purpose, room temperature curing, epoxy adhesive and sealant. Flexibility can be adjusted .. |
|||
Adhesive Bond Strength | 16.5 MPa @Temperature -54.4 °C |
2400 psi @Temperature -66.0 °F |
Aluminum-Aluminum tensile shear |
Armstrong A-1/A Epoxy Adhesive A brown epoxy paste formulated with enhanced wetting capabilities to hard rubbers and rigid thermoplastics. Has low outgassing characteristics at temperatures below 250°FInformation provided by El.. |
|||
Adhesive Bond Strength | 16.5 MPa @Temperature 25.0 °C |
2400 psi @Temperature 77.0 °F |
Aluminum-Aluminum tensile shear |
Armstrong A-1/A Epoxy Adhesive A brown epoxy paste formulated with enhanced wetting capabilities to hard rubbers and rigid thermoplastics. Has low outgassing characteristics at temperatures below 250°FInformation provided by El.. |
|||
Adhesive Bond Strength | 16.5 MPa @Temperature 82.2 °C |
2400 psi @Temperature 180 °F |
Aluminum-Aluminum tensile shear |
Armstrong A-4/E Epoxy Adhesive Is a heavy, non-metallic filled, gray paste epoxy that provides excellent thixotropic non-sag bond lines. It can be used for small volume casting applications.Information provided by Ellsworth Adhe.. |
|||
Adhesive Bond Strength | 16.5 MPa @Temperature -54.4 °C |
2400 psi @Temperature -66.0 °F |
Aluminum-Aluminum tensile shear |
Armstrong A-4/E Epoxy Adhesive Is a heavy, non-metallic filled, gray paste epoxy that provides excellent thixotropic non-sag bond lines. It can be used for small volume casting applications.Information provided by Ellsworth Adhe.. |