Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Glass Transition Temp, Tg 92.0 °C
198 °F
TM R050-25
Resinlab® EP1330 Heat Cure Epoxy Polymer System
Resinlab™ EP1330 and EP1330LV are one part heat cure epoxy polymer systems. They can also be used as a small mass potting or staking compounds, or a dam adhesive in and “dam and fill” application..
Glass Transition Temp, Tg 92.0 °C
198 °F
TM R050-25
Resinlab® EP1385 Black Epoxy Formulation
Resinlab™ EP1385 Black is an epoxy formulation designed for applications requiring resistance to E-85 type fuels. It has good wetting and adhesion to most surfaces. It has very good resistance to w..
Glass Transition Temp, Tg 92.0 °C
198 °F
TM R050-25
Resinlab® EP1385 Clear Epoxy Formulation
Resinlab™ EP1385 Clear is an epoxy formulation designed for applications requiring resistance to E-85 type fuels. It has good wetting and adhesion to most surfaces. It has very good resistance to w..
Glass Transition Temp, Tg 92.0 °C
198 °F
DSC
Solvay Specialty Polymers Ajediumâ„¢ Films PPS Polyphenylene Sulfide (PPS)
Polyphenylene sulfide, PPS, is a thermoplastic film that has excellent chemical resistance and good electrical and physical properties.Features: Flame Retardant; Good Chemical Resistance; Good Elect..
Glass Transition Temp, Tg 92.0 °C
198 °F
Ultimate Tg
Tra-Con Tra-Bond 7560D Hydrolytically Stable Adhesive
TRA-BOND 7560D is an electrically insulating epoxy adhesive. This material has a 10 day work life and a medium viscosity for easy usage. There are also multiple cure options that make this product i..
Glass Transition Temp, Tg 92.0 °C
198 °F
Ultimate Tg
Tra-Con Tra-Duct 2958 Snap Cure Conductive Silver Epoxy Adhesive
TRA-DUCT 2958 is a two-part, smooth paste of specially refined and processed epoxy and silver components, recommended for electronic, microelectronic and die-attach bonding and sealing applications ..
Glass Transition Temp, Tg 92.0 °C
198 °F
Ultimate Tg
Tra-Con Tra-Duct 2924 Conductive Silver Epoxy Adhesive
TRA-DUCT 2924 is a two part electrically conductive composition developed for low shrinkage, low resistivity bonding applications where good electrical and physical properties over a wide temperatur..
Glass Transition Temp, Tg 92.0 °C
198 °F
Armstrong X-6/E Epoxy Adhesive
Thixotropic.Information provided by Ellsworth Adhesives.
Glass Transition Temp, Tg 92.0 °C
198 °F
Atom Adhesives AA-DUCT 2924 Epoxy Adhesive
AA-DUCT 2924 is a two part electrically conductive composition developed for low shrinkage; low resistivity bonding applications where good electrical and physical properties over a wide temperature..
Glass Transition Temp, Tg 92.0 °C
198 °F
Eastman Eastalloy DA107 PC+PET Copolyester/Polycarbonate  (discontinued **)
ISO data as provided by the manufacturer, Eastman Chemical