Thermal Properties | Metric | English | Comments |
---|---|---|---|
Glass Transition Temp, Tg | 92.0 °C | 198 °F | TM R050-25 |
Resinlab® EP1330 Heat Cure Epoxy Polymer System Resinlab™ EP1330 and EP1330LV are one part heat cure epoxy polymer systems. They can also be used as a small mass potting or staking compounds, or a dam adhesive in and “dam and fill” application.. |
|||
Glass Transition Temp, Tg | 92.0 °C | 198 °F | TM R050-25 |
Resinlab® EP1385 Black Epoxy Formulation Resinlab™ EP1385 Black is an epoxy formulation designed for applications requiring resistance to E-85 type fuels. It has good wetting and adhesion to most surfaces. It has very good resistance to w.. |
|||
Glass Transition Temp, Tg | 92.0 °C | 198 °F | TM R050-25 |
Resinlab® EP1385 Clear Epoxy Formulation Resinlab™ EP1385 Clear is an epoxy formulation designed for applications requiring resistance to E-85 type fuels. It has good wetting and adhesion to most surfaces. It has very good resistance to w.. |
|||
Glass Transition Temp, Tg | 92.0 °C | 198 °F | DSC |
Solvay Specialty Polymers Ajediumâ„¢ Films PPS Polyphenylene Sulfide (PPS) Polyphenylene sulfide, PPS, is a thermoplastic film that has excellent chemical resistance and good electrical and physical properties.Features: Flame Retardant; Good Chemical Resistance; Good Elect.. |
|||
Glass Transition Temp, Tg | 92.0 °C | 198 °F | Ultimate Tg |
Tra-Con Tra-Bond 7560D Hydrolytically Stable Adhesive TRA-BOND 7560D is an electrically insulating epoxy adhesive. This material has a 10 day work life and a medium viscosity for easy usage. There are also multiple cure options that make this product i.. |
|||
Glass Transition Temp, Tg | 92.0 °C | 198 °F | Ultimate Tg |
Tra-Con Tra-Duct 2958 Snap Cure Conductive Silver Epoxy Adhesive TRA-DUCT 2958 is a two-part, smooth paste of specially refined and processed epoxy and silver components, recommended for electronic, microelectronic and die-attach bonding and sealing applications .. |
|||
Glass Transition Temp, Tg | 92.0 °C | 198 °F | Ultimate Tg |
Tra-Con Tra-Duct 2924 Conductive Silver Epoxy Adhesive TRA-DUCT 2924 is a two part electrically conductive composition developed for low shrinkage, low resistivity bonding applications where good electrical and physical properties over a wide temperatur.. |
|||
Glass Transition Temp, Tg | 92.0 °C | 198 °F | |
Armstrong X-6/E Epoxy Adhesive Thixotropic.Information provided by Ellsworth Adhesives. |
|||
Glass Transition Temp, Tg | 92.0 °C | 198 °F | |
Atom Adhesives AA-DUCT 2924 Epoxy Adhesive AA-DUCT 2924 is a two part electrically conductive composition developed for low shrinkage; low resistivity bonding applications where good electrical and physical properties over a wide temperature.. |
|||
Glass Transition Temp, Tg | 92.0 °C | 198 °F | |
Eastman Eastalloy DA107 PC+PET Copolyester/Polycarbonate
(discontinued **) ISO data as provided by the manufacturer, Eastman Chemical |