Tra-Con Tra-Bond 546S01 Low Viscosity UV Curable Adhesive

Category Polymer , Adhesive , Thermoset
Manufacturer Tra-Con, Inc.
Trade Name Tra-Bond
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Tra-Con Tra-Bond 546S01 Low Viscosity UV Curable Adhesive.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
TRA-BOND 546S01 is a low viscosity UV curable adhesive with a secondary heat curing system to achieve a high Tg. It exhibits excellent adhesion to glass and many other substrates, making it ideal for a wide variety of optical applications. The 546S01 also has low cure shrinkage to minimize stress. An additional post heat cure at 100-130°C is required to achieve ultimate properties.Information provided by Tra-Con Inc.
Physical Properties Metric English Comments
Specific Gravity 1.00 g/cc
1.00 g/cc
Cured
Viscosity 1000 cP
1000 cP
Mixed (cp #40, 10 rpm)
Mechanical Properties Metric English Comments
Hardness, Shore D 87
87
Thermal Properties Metric English Comments
CTE, linear 68.0 µm/m-°C

@Temperature 20.0 °C
37.8 µin/in-°F

@Temperature 68.0 °F
Glass Transition Temp, Tg 88.0 °C
190 °F
Ultimate Tg; TMA
Shrinkage 0.30 %
0.30 %
Linear, UV only
1.3 %
1.3 %
Linear, UV plus heat
Processing Properties Metric English Comments
Cure Time 0.167 - 0.500 min
0.00278 - 0.00833 hour
350-380nm
Descriptive Properties Value Comments
Color Transparent