Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear | 68.0 µm/m-°C @Temperature -30.0 - 80.0 °C |
37.8 µin/in-°F @Temperature -22.0 - 176 °F |
ASTM E228 |
Solvay Engineered Polymers SEQUEL® 5220 Engineered Polyolefin
(discontinued **) Description: SEQUEL® 5220 engineered polyolefin is designed for large exterior applications that require superior painted gouge/scuff performance. This product also offers ductile impact propertie.. |
|||
CTE, linear | 68.0 - 110 µm/m-°C | 37.8 - 61.1 µin/in-°F | Average value: 87.8 µm/m-°C Grade Count:28 |
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), Extruded This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS), Extruded". Each property range of values reported is minimum and .. |
|||
CTE, linear | 68.0 µm/m-°C @Temperature -40.0 - 82.0 °C |
37.8 µin/in-°F @Temperature -40.0 - 180 °F |
ASTM D696 |
LG Chemical Lupoy 1200-10 Polycarbonate Resin Description: LUPOY PC 1200-10 resin is designed for extrusion and injection molding products. It exhibits an excellent physical property balance of heat resistance, transparency and impact strength... |
|||
CTE, linear | 68.0 µm/m-°C @Temperature -40.0 - 82.0 °C |
37.8 µin/in-°F @Temperature -40.0 - 180 °F |
ASTM D696 |
LG Chemical Lupoy 1200-22 Polycarbonate Resin Description: LUPOY PC 1200-22 resin is designed for extrusion and injection molding products. It exhibits an excellent physical property balance of heat resistance, transparency and impact strength... |
|||
CTE, linear | 68.0 µm/m-°C @Temperature -40.0 - 82.0 °C |
37.8 µin/in-°F @Temperature -40.0 - 180 °F |
ASTM D696 |
LG Chemical Lupoy 1301-10 Polycarbonate Resin Description: LUPOY PC 1301-10 resin is designed for extrusion and injection molding products. It exhibits an excellent physical property balance of heat resistance, transparency and impact strength... |
|||
CTE, linear | 68.0 µm/m-°C @Temperature -40.0 - 82.0 °C |
37.8 µin/in-°F @Temperature -40.0 - 180 °F |
ASTM D696 |
LG Chemical Lupoy 1301EP-22 Polycarbonate Resin Description: LUPOY PC 1301EP-22 resin is designed for extrusion and injection molding products. It exhibits an excellent physical property balance of heat resistance, transparency and impact strengt.. |
|||
CTE, linear | 68.0 µm/m-°C @Temperature -40.0 - 82.0 °C |
37.8 µin/in-°F @Temperature -40.0 - 180 °F |
ASTM D696 |
LG Chemical Lupoy 1301EP30 Polycarbonate Resin Description: LUPOY PC 1301EP-30 resin is designed for extrusion and injection molding products. It exhibits an excellent physical property balance of heat resistance, transparency and impact strengt.. |
|||
CTE, linear | 68.0 µm/m-°C @Temperature -40.0 - 82.0 °C |
37.8 µin/in-°F @Temperature -40.0 - 180 °F |
ASTM D696 |
LG Chemical Lupoy 1261-03 Polycarbonate Resin Description: LUPOY PC 1261-03 resin is designed for extrusion blow molding(EBM) and injection stretch blow molding (ISBM) products. It exhibits an excellent physical property balance of heat resista.. |
|||
CTE, linear | 68.0 µm/m-°C @Temperature -40.0 - 82.0 °C |
37.8 µin/in-°F @Temperature -40.0 - 180 °F |
ASTM D696 |
LG Chemical Lupoy 1302-07 Polycarbonate Resin Description: LUPOY PC 1302-07 resin is designed for extrusion and injection molding products. It exhibits an excellent physical property balance of heat resistance, transparency and impact strength... |
|||
CTE, linear | 68.0 µm/m-°C @Temperature -40.0 - 82.0 °C |
37.8 µin/in-°F @Temperature -40.0 - 180 °F |
ASTM D696 |
LG Chemical Lupoy 1303EP-22 Polycarbonate Resin Description: LUPOY PC 1303EP-22 resin is designed for extrusion and injection molding products. It exhibits an excellent physical property balance of heat resistance, transparency and impact strengt.. |
|||
CTE, linear | 68.0 µm/m-°C @Temperature -40.0 - 82.0 °C |
37.8 µin/in-°F @Temperature -40.0 - 180 °F |
ASTM D696 |
LG Chemical Lupoy 1621-02 Polycarbonate Resin Description: LUPOY PC 1621-02 resin is designed for large injection stretch blow molding and extrusion blow molding parts. It exhibits an excellent physical property balance of heat resistance, tran.. |
|||
CTE, linear | 68.0 µm/m-°C @Temperature -40.0 - 82.0 °C |
37.8 µin/in-°F @Temperature -40.0 - 180 °F |
ASTM D696 |
LG Chemical Lupoy 3010-10 Polycarbonate Resin Description: LUPOY PC 3010-10 resin is designed for injection molding products. It exhibits an excellent physical property balance of heat resistance, transparency and impact strength.Main Character.. |
|||
CTE, linear | 68.0 µm/m-°C @Temperature -40.0 - 82.0 °C |
37.8 µin/in-°F @Temperature -40.0 - 180 °F |
ASTM D696 |
LG Chemical Lupoy 3030-15 Polycarbonate Resin Description: LUPOY PC 3030-15 resin is designed for injection molding products. It exhibits an excellent physical property balance of heat resistance, transparency and impact strength.Main Character.. |
|||
CTE, linear | 68.0 µm/m-°C @Temperature -40.0 - 82.0 °C |
37.8 µin/in-°F @Temperature -40.0 - 180 °F |
ASTM D696 |
LG Chemical Lupoy NF1005F 03R Polycarbonate Resin Description: LUPOY NF 1005F03R, eco-friendly UL94 V0/1.5 mm, is designed for extrusion products. It combines an excellent physical property balance of heat resistance, transparency and impact streng.. |
|||
CTE, linear | 68.0 µm/m-°C @Temperature -40.0 - 82.0 °C |
37.8 µin/in-°F @Temperature -40.0 - 180 °F |
ASTM D696 |
LG Chemical Lupoy NF1009F 15 Polycarbonate Resin Description: LUPOY NF 1009F15, eco-friendly UL94 V0/2.0 mm, is designed for extrusion and injection molding products. It combines an excellent physical property balance of heat resistance, transpare.. |
|||
CTE, linear | 68.0 µm/m-°C | 37.8 µin/in-°F | DIN 52328 |
Isoflon PMMA Polymethyl-methacrylate Products with good mechanical performances under friction and good dimensional stability, notably in moist environmentsVery rigid, hardHigh machining precisionInformation provided by Isoflon. |
|||
CTE, linear | 68.0 µm/m-°C @Temperature -40.0 - 82.0 °C |
37.8 µin/in-°F @Temperature -40.0 - 180 °F |
ASTM D696 |
LG Chemical Lupoy 1201HP-08 Polycarbonate Resin Description: LUPOY PC 1201HP-08 resin is designed for extrusion and injection molding products. It exhibits an excellent physical property balance of heat resistance, transparency and impact strengt.. |
|||
CTE, linear | 68.0 µm/m-°C @Temperature -40.0 - 82.0 °C |
37.8 µin/in-°F @Temperature -40.0 - 180 °F |
ASTM D696 |
LG Chemical Lupoy 1201HP-21 Polycarbonate Resin Description: LUPOY PC 1201HP-21 resin is designed for extrusion and injection molding products. It exhibits an excellent physical property balance of heat resistance, transparency and impact strengt.. |
|||
CTE, linear | 68.0 µm/m-°C @Temperature -40.0 - 82.0 °C |
37.8 µin/in-°F @Temperature -40.0 - 180 °F |
ASTM D696 |
LG Chemical Lupoy 1300-10 Polycarbonate Resin Description: LUPOY PC 1300-10 resin is designed for extrusion and injection molding products. It exhibits an excellent physical property balance of heat resistance, transparency and impact strength... |
|||
CTE, linear | 68.0 µm/m-°C @Temperature -40.0 - 82.0 °C |
37.8 µin/in-°F @Temperature -40.0 - 180 °F |
ASTM D696 |
LG Chemical Lupoy 1300-12 Polycarbonate Resin Description: LUPOY PC 1300-12 resin is designed for extrusion and injection molding products. It exhibits an excellent physical property balance of heat resistance, transparency and impact strength... |
|||
CTE, linear | 68.0 µm/m-°C @Temperature 20.0 °C |
37.8 µin/in-°F @Temperature 68.0 °F |
ASTM D696 |
Ineos ABS Lustran® SAN Sparkle Highest-Clarity |
|||
CTE, linear | 68.0 µm/m-°C @Temperature -40.0 - 82.0 °C |
37.8 µin/in-°F @Temperature -40.0 - 180 °F |
ASTM D696 |
LG Chemical Lupoy 1303-07 Polycarbonate Resin Description: LUPOY PC 1303-07 resin is designed for extrusion and injection molding products. It exhibits an excellent physical property balance of heat resistance, transparency and impact strength... |
|||
CTE, linear | 68.0 µm/m-°C @Temperature -40.0 - 82.0 °C |
37.8 µin/in-°F @Temperature -40.0 - 180 °F |
ASTM D696 |
LG Chemical Lupoy 1303AH-10 Polycarbonate Resin Description: LUPOY PC 1303AH-10 Tint Polycarbonate Resin is designed for injection molding of auto-headlamps. It exhibits an excellent physical property balance of heat resistance, transparency and .. |
|||
CTE, linear | 68.0 µm/m-°C @Temperature -40.0 - 82.0 °C |
37.8 µin/in-°F @Temperature -40.0 - 180 °F |
ASTM D696 |
LG Chemical Lupoy 1303EP-30 Polycarbonate Resin Description: LUPOY PC 1303EP-30 resin is designed for extrusion and injection molding products. It exhibits an excellent physical property balance of heat resistance, transparency and impact strengt.. |
|||
CTE, linear | 68.0 µm/m-°C @Temperature -30.0 - 80.0 °C |
37.8 µin/in-°F @Temperature -22.0 - 176 °F |
Borealis Method |
Borealis Daplen™ EH104AE Polypropylene TPO Compound Daplen™ EH104AE is a 10% mineral filled elastomer modified polypropylene compound intended for injection molding. This material has an excellent balance between impact strength and stiffness, high.. |
|||
CTE, linear | 68.0 µm/m-°C | 37.8 µin/in-°F | Below Tg |
Tra-Con Tra-Bond 221N01 Information provided by Tra-Con Inc. |
|||
CTE, linear | 68.0 µm/m-°C @Temperature 20.0 °C |
37.8 µin/in-°F @Temperature 68.0 °F |
|
Tra-Con Tra-Bond 546S01 Low Viscosity UV Curable Adhesive TRA-BOND 546S01 is a low viscosity UV curable adhesive with a secondary heat curing system to achieve a high Tg. It exhibits excellent adhesion to glass and many other substrates, making it ideal fo.. |
|||
CTE, linear | 68.0 µm/m-°C @Temperature 20.0 °C |
37.8 µin/in-°F @Temperature 68.0 °F |
ASTM D696 |
Devcon Plastic Steel® Liquid (B) Epoxy General Repair EpoxyComments: Steel-filled liquid epoxy can be cast over models for accurate detail reproduction when making holding fixtures, light-gauge forming dies and molds. Hardens in about a.. |
|||
CTE, linear | 68.0 µm/m-°C | 37.8 µin/in-°F | Below Tg |
Epoxy Technology EPO-TEK® T7109-18 Electrically Insulating Epoxy Paste Material Description: A flexible, electrically insulating epoxy paste designed for low stress and heat dissipation applications. Alternative to EPO-TEK® T7109-17.Information Provided by Epoxy Tec.. |
|||
CTE, linear | 68.0 µm/m-°C @Temperature -40.0 - 82.0 °C |
37.8 µin/in-°F @Temperature -40.0 - 180 °F |
ASTM D696 |
LG Chemical Lupoy 1302HP-07 Polycarbonate Resin Description: LUPOY PC 1302HP-07 resin is designed for extrusion products. It exhibits an excellent physical property balance of heat resistance, transparency and impact strength.Main Characteristics.. |