Thermal Properties | Metric | English | Comments |
---|---|---|---|
Glass Transition Temp, Tg | 88.0 °C | 190 °F | |
Chevron Phillips Ryton® A-200 PPS Polyphenylene Sulfide
(discontinued **) Ryton® PPS is used in many electronic and automotive applications because of its high strength, favorable electrical properties, and high temperature stability.Data provided by the manufacturer.Sol.. |
|||
Glass Transition Temp, Tg | 88.0 °C | 190 °F | |
Chevron Phillips Ryton® R-4 06 PPS (Polyphenylene Sulfide)
(discontinued **) Ryton® PPS is used in many electronic and automotive applications because of its high strength, favorable electrical properties, and high temperature stability.Data provided by the manufacturer.Sol.. |
|||
Glass Transition Temp, Tg | 88.0 °C | 190 °F | |
Chevron Phillips Ryton® R10 5002C PPS Polyphenylene Sulfide
(discontinued **) Ryton® PPS is used in many electronic and automotive applications because of its high strength, favorable electrical properties, and high temperature stability.Data provided by the manufacturer.Sol.. |
|||
Glass Transition Temp, Tg | 88.0 °C | 190 °F | |
Chevron Phillips Ryton® R10 5004A PPS Polyphenylene Sulfide
(discontinued **) Ryton® PPS is used in many electronic and automotive applications because of its high strength, favorable electrical properties, and high temperature stability.Data provided by the manufacturer.Sol.. |
|||
Glass Transition Temp, Tg | 88.0 °C | 190 °F | Ultimate Tg; TMA |
Tra-Con Tra-Bond 546S01 Low Viscosity UV Curable Adhesive TRA-BOND 546S01 is a low viscosity UV curable adhesive with a secondary heat curing system to achieve a high Tg. It exhibits excellent adhesion to glass and many other substrates, making it ideal fo.. |
|||
Glass Transition Temp, Tg | 88.0 °C | 190 °F | Ultimate Tg, cured 1 hr @ 150°C |
Tra-Con Tra-Duct 8205 One-Part Electrically Conductive Silver-Filled Epoxy TRA-DUCT 8205 is an electrically conducting silver-filled epoxy compound recommended for electronic bonding and sealing applications that require a combination of excellent mechanical and electrical.. |
|||
Glass Transition Temp, Tg | 88.0 °C | 190 °F | by DMTA following AITM 1-0003. Higher Tg possible by adjustment of cure time. |
Hexcel® HexMC™ C / 2000 / R1 Composite SMC High performance sheet-molding compound, specifically designed for compression molding. The epoxy matrix and high carbon fiber volume enable components to be molded for a wide range of applications.. |
|||
Glass Transition Temp, Tg | 88.0 °C | 190 °F | Wet |
Hexcel® HexPly® F522 Epoxy Resin HexPly® F522 is an advanced, modified epoxy formulation designed for autoclave curing to offer very high laminate strengths, coupled with increased fracture toughness, excellent hot-wet properties .. |
|||
Glass Transition Temp, Tg | 88.0 °C | 190 °F | |
Epoxyset Epoxiohm EO-24 Electrically Conductive Epoxy Adhesive EO-24 is a two components, 100% solids silver-filled epoxy system designed specifically for chip bonding in microelectronic and optoelectronic applications. It is used for thermal management applica.. |
|||
Glass Transition Temp, Tg | 88.0 °C | 190 °F | dynamic; DIN 53 736 |
Hippe PPS High hardness and stiffness, good abrasion resistance, low moisture absorption, favorable insulating features, low dielectric, high non-inflammability and high chemical resistance are the essential .. |
|||
Glass Transition Temp, Tg | 88.0 °C | 190 °F | |
Chevron Phillips Ryton® R10 7006A PPS Polyphenylene Sulfide
(discontinued **) Ryton® PPS is used in many electronic and automotive applications because of its high strength, favorable electrical properties, and high temperature stability.Data provided by the manufacturer.Sol.. |
|||
Glass Transition Temp, Tg | 88.0 - 90.0 °C | 190 - 194 °F | Average value: 89.6 °C Grade Count:5 |
Overview of materials for Polyphenylene Sulfide (PPS), Unreinforced, Extruded This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Sulfide (PPS), Unreinforced, Extruded". Each property range of values reported is minimum .. |
|||
Glass Transition Temp, Tg | 88.0 °C | 190 °F | |
Chevron Phillips Ryton® R-4 04 PPS (Polyphenylene Sulfide)
(discontinued **) Ryton® PPS is used in many electronic and automotive applications because of its high strength, favorable electrical properties, and high temperature stability.Data provided by the manufacturer.Sol.. |
|||
Glass Transition Temp, Tg | 88.0 °C | 190 °F | |
Solvay Specialty Polymers Amodel® A-6625 HS BK324 Polyphthalamide, 25% carbon/glass fiber, ESD grade
(discont Amodel A-6625 HS BK324 is a 25% carbon and glass-fiber-reinforced, heat-stabilized grade of polyphthalamide (PPA). It is formulated for applications requiring the dissipation of static charge. This .. |