Thermal Properties | Metric | English | Comments |
---|---|---|---|
Deflection Temperature at 0.46 MPa (66 psi) | 105 °C | 221 °F | ASTM D648 |
SABIC PP 49MK45 Polypropylene Impact Copolymer for Injection Molding Product Description: PP 49MK45 is specially developed for producing injection molded articles. This grade contains an antistatic & nucleating agents. It has medium flow properties, good impact re.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 105 °C | 221 °F | 120°C/h; ISO 75/1 |
Polykemi AB POLYblend 45FS PC/ABS-blend, Flame Retardant Information provided by Polykemi AB |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 105 °C @Thickness 3.20 mm |
221 °F @Thickness 0.126 in |
unannealed; ASTM D648 |
SABIC Innovative Plastics Lexan® BPL1000 PC (Europe-Africa-Middle East) Lexan* BPL1000 Polycarbonate (PC) resin is an injection moldable grade featuring high flow and good impact peroformance. It contains non-chlorinated and non-brominated flame retardant systems with U.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 105 °C | 221 °F | ASTM D648 |
Reliance Industries Repol B220MN Polypropylene REPOL Polypropylene B220MN is manufactured using Unipol PP process which combines the production efficiency of gas phase fluidized bed reactor technology with the high activity stereospecific cataly.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 105 °C | 221 °F | ASTM D648 |
Reliance Industries Repol B400MN Polypropylene REPOL Polypropylene B400MN is manufactured using Unipol PP process which combines the production efficiency of gas phase fluidized bed reactor technology with the high activity stereospecific cataly.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 105 °C | 221 °F | ASTM D648 |
LG Chemical SEETEC M1500 Polypropylene Impact Copolymer SEETEC M1500 is a heterophasic polypropylene copolymer for injection molding applications. SEETEC M1500 exhibits a high flowability and a good balance of stiffness and impact strength. SEETEC M1500 .. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 105 °C | 221 °F | ISO 75-1,-2 |
Inno-Comp INNOPOL® CS 2-9000 Polypropylene Block-Copolymer INNOPOL® CS 2-9000 is a polypropylene block-copolymer based compound. This grade is available in nature and custom colored form.INNOPOL® CS 2-9000 is developed for producing injection molded a.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 105 - 110 °C | 221 - 230 °F | ASTM D1525, HDT Method B |
Loxim 820 02C HB Polypropylene Compound, 20% Calcite Filled, Flame Retardant Information provided by Loxim Industries |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 105 - 110 °C | 221 - 230 °F | ASTM D1525, HDT Method B |
Loxim 821 02T HB Polypropylene Compound, 20% Talc Filled, Flame Retardant Information provided by Loxim Industries |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 105 °C | 221 °F | Edgew 120*10*4 sp=100mm; ISO 75/Be |
SABIC Innovative Plastics Xenoy® 5220U PBT+PC (Europe-Africa-Middle East) Unreinforced PBT+PC alloy. Improved retention of mechanical properties under UV. Excellent low temperature/chemical |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 105 °C | 221 °F | Edgew 120*10*4 sp=100mm; ISO 75/Be |
SABIC Innovative Plastics Xenoy® CL402 PBT+PC (Asia Pacific) XENOY CL402 is a high viscosity, unfilled, elastomer modified PC/PBT blend for extrusion/blowmolding applications. ISO1043-label: PC+PBT-I.This data was supplied by SABIC-IP for the Asia Pacific reg.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 105 °C | 221 °F | Flatw 80*10*4 sp=64mm; ISO 75/Bf |
SABIC Innovative Plastics LNP Thermocomp AF0029 ABS LNP* Thermocomp* AF0029 is an ABS base resin containing Glass Fiber. Characteristics of this grade are Flame Retardancy.This data was supplied by SABIC-IP for the Americas region. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 105 °C | 221 °F | ASTM D648 |
SK Chemicals SKYPEL G155D General Grade SKYPEL is a thermoplastic polyester elastomer (TPEE). It is a polymer resin having the property somewhere between plastics and rubber, which have various properties ranging from high hardness plasti.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 105 °C | 221 °F | Edgew 120*10*4 sp=100mm; ISO 75/Be |
SABIC Innovative Plastics Xenoy® XD1507S PBT+PC (Europe-Africa-Middle East) XENOY XD1507S is an impact modified PBT+PC blend with outstanding chemical resistance, good UV stability and flow properties, designed for self coloured, optiwall bumper facias.This data was supplie.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 105 °C | 221 °F | Unannealed; ASTM Data |
Styron Magnum™ 358HP ABS, High Heat MAGNUM® ABS resins are thermoplastic materials which provide an excellent balance of processability, impact resistance and heat resistance as imparted by the various polymer compositions. MAGNUM .. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 105 °C | 221 °F | ASTM D648 |
SK Chemicals SKYPEL G455D Special Grade Oil-Resistant Grade SKYPEL is a thermoplastic polyester elastomer (TPEE). It is a polymer resin having the property somewhere between plastics and rubber, which have various properties ranging from high hardness plasti.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 105 °C | 221 °F | ASTM D648 |
A. Schulman POLYFORT™ PP 3153 Homopolymer Polypropylene DescriptionPolyfort® PP 3153 is a homopolymer polypropylene.Information provided by A. Schulman. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 105 °C | 221 °F | ASTM D648 |
A. Schulman POLYFORT™ FPP 4529 Mineral Filled Copolymer Polypropylene DescriptionPolyfort® FPP 4528 is a mineral filled copolymer polypropylene for applications requiring good impact and increased stiffness with long term heat stability.Information provided by A. Sch.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 105 °C | 221 °F | ASTM D648 |
A. Schulman POLYFORT™ FPP 1697HU High Flow Fortified Polypropylene DescriptionPolyfort® FPP 1697HU is a high flow fortified polypropylene with high temperature dimensioned stability. It is stabilized for UV exposure and available in matched automotive color.Infor.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 105 °C | 221 °F | ASTM D648 |
A. Schulman POLYFORT™ FPP 4529 Mineral Filled Copolymer Polypropylene DescriptionPolyfort® FPP 4528 is a mineral filled copolymer polypropylene for applications requiring good impact and increased stiffness with long term heat stability.Information provided by A. Sch.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 105 °C | 221 °F | 120°C per hour; ISO 75-2 |
Total PPH 4042 Polypropylene, Homopolymer ATOFINA Polypropylene PPH 4042 is a nucleated homopolymer.ApplicationATOFINA Polypropylene PPH 4042 has been developed for extrusion-thermoforming, providing improved rigidity and impact resistance .. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 105 °C | 221 °F | ASTM D648 |
A. Schulman POLYFORT™ FPP 3391 Chemically Coupled, Modified Polypropylene DescriptionPolyfort® FPP 3391 is a chemically coupled, mineral reinforced high impact resistant, modified polypropylene.Information provided by A. Schulman. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 105 °C | 221 °F | ASTM D648 |
A. Schulman POLYFORT™ FPP 1237 CaCO3 filled homopolymer polypropylene DescriptionPolyfort® FPP 1237 is a 20% CAC03 filled homopolymer polypropylene product. Information provided by A. Schulman. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 105 °C | 221 °F | ISO 75-1/-2 |
EMS-Grivory Grivory® TR XE 4010 PA*-I Product description: Grilamid XE 4010 is an amorphous cycloaliphatic copolyamide based on 58 % renewable resources. The material is designed for applications where high chemical resistance, high fat.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 105 °C | 221 °F | ASTM D648 |
Entec Hypro™ PP-CP20/10 Impact Copolymer, 20 Melt Flow This product is intended for general purpose injection molding applications including flooring, automotive, appliance, lawn and garden and industrial application.Information provided by Entec |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 105 °C | 221 °F | ASTM D648 |
Entec Hypro™ PP-HP12 Homopolymer, 12 Melt Flow This product in intended for general purpose injection molding applications such as caps and closures, resin furniture and consumer products.Information provided by Entec |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 105 °C | 221 °F | ISO 75 |
Eurotec® Tecotek® PC30 NL TD 700 PC, unfilled, flame retardant - halogen (RoHS compliant), impact modified, natural Information provided by Eurotec® |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 105 °C | 221 °F | ASTM D648 |
Carmel Olefins CAPILENE® HT 75 A Polypropylene Impact Copolymer Description: CAPILENE® HT 75 A is a nucleated and antistatic high flow impact copolymer for injection molding. It is characterized by improved stiffness, medium impact resistance and good organol.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 105 °C | 221 °F | 120°C/h; ISO 75/1 |
Polykemi AB POLYabs F20 GF17 ABS, Glass Fiber Reinforced Information provided by Polykemi AB |