Material Notes:
Availability: Africa & Middle East; Latin America; Asia Pacific; South America Talc Filler, 30% Filler by Weight Uses: Appliance Components; Automotive Applications; Housings Forms: Pellets Processing Method: Injection MoldingInformation Provided by Teknor Apex
Physical Properties Metric English Comments
Specific Gravity 1.11 g/cc
1.11 g/cc
ASTM D792
Linear Mold Shrinkage 0.0080 cm/cm
0.0080 in/in
ASTM D955
Melt Flow 11.0 g/10 min

@Load 2.16 kg,
Temperature 230 °C
11.0 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength, Yield 29.0 MPa
4210 psi
ASTM D638
Elongation at Break 48 %
48 %
ASTM D412
Flexural Strength 39.0 MPa
5660 psi
ASTM D790
Flexural Modulus 2.23 GPa
323 ksi
ASTM D790
Izod Impact, Notched 0.491 J/cm

@Temperature 22.8 °C
0.920 ft-lb/in

@Temperature 73.0 °F
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 129 °C
264 °F
Unannealed; ASTM D648
Vicat Softening Point 152 °C
306 °F
Loading 1 (10 N); ASTM D1525
Copyright © lookpolymers.com All Rights Reserved