Physical Properties | Metric | English | Comments |
---|---|---|---|
Melt Flow | 11.0 - 35.0 g/10 min | 11.0 - 35.0 g/10 min | Average value: 20.1 g/10 min Grade Count:7 |
Overview of materials for ABS/Polyester Alloy This property data is a summary of similar materials in the MatWeb database for the category "ABS/Polyester Alloy". Each property range of values reported is minimum and maximum values of appropriat.. |
|||
Melt Flow | 11.0 g/10 min @Load 2.16 kg, Temperature 190 °C |
11.0 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
Teknor Apex Monprene® MP-2250 Thermoplastic Elastomer Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo.. |
|||
Melt Flow | 11.0 g/10 min @Load 5.00 kg, Temperature 200 °C |
11.0 g/10 min @Load 11.0 lb, Temperature 392 °F |
ASTM D1238 |
Teknor Apex Monprene® MP 1056 Thermoplastic Elastomer Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo.. |
|||
Melt Flow | 11.0 g/10 min @Load 10.0 kg, Temperature 190 °C |
11.0 g/10 min @Load 22.0 lb, Temperature 374 °F |
ASTM D1238 |
Teknor Apex Sinpolene MBB005LE Low Density Polyethylene Availability: Africa & Middle East; Latin America; Asia Pacific; South America Additive: Carbon Black (380000 ppm) Features: General Purpose Uses: Film Forms: Pellets Processing Method: Blow Moldi.. |
|||
Melt Flow | 11.0 g/10 min @Load 2.16 kg, Temperature 230 °C |
11.0 g/10 min @Load 4.76 lb, Temperature 446 °F |
ASTM D1238 |
Teknor Apex Sinpolene TPP1020 Polypropylene Availability: Africa & Middle East; Latin America; Asia Pacific; South America Talc Filler, 20% Filler by Weight Uses: Automotive Applications; Housings Forms: Pellets Processing Method: Injection .. |
|||
Melt Flow | 11.0 g/10 min @Load 2.16 kg, Temperature 230 °C |
11.0 g/10 min @Load 4.76 lb, Temperature 446 °F |
ASTM D1238 |
Teknor Apex Telcar® OBC 4965F Thermoplastic Elastomer Notes: Telcar OBC has superior mechanical strength and higher elongation which will provide a tougher more durable finished product. Telcar OBC can be used in less demanding sealing applications. T.. |
|||
Melt Flow | 11.0 g/10 min @Load 2.16 kg, Temperature 230 °C |
11.0 g/10 min @Load 4.76 lb, Temperature 446 °F |
ASTM D1238 |
Teknor Apex Telcar® TL-1140E Thermoplastic Elastomer Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets P.. |
|||
Melt Flow | 11.0 g/10 min @Load 2.16 kg, Temperature 230 °C |
11.0 g/10 min @Load 4.76 lb, Temperature 446 °F |
ASTM D1238 |
Teknor Apex Telcar® TL-1155B Thermoplastic Elastomer Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets P.. |
|||
Melt Flow | 11.0 g/10 min @Load 2.16 kg, Temperature 230 °C |
11.0 g/10 min @Load 4.76 lb, Temperature 446 °F |
ASTM D1238 |
Teknor Apex Telcar® TL-355 Thermoplastic Elastomer Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets .. |
|||
Melt Flow | 11.0 g/10 min @Load 2.16 kg, Temperature 230 °C |
11.0 g/10 min @Load 4.76 lb, Temperature 446 °F |
ASTM D1238 |
Teknor Apex Sinpolene TPP2030 Polypropylene Availability: Africa & Middle East; Latin America; Asia Pacific; South America Talc Filler, 30% Filler by Weight Uses: Appliance Components; Automotive Applications; Housings Forms: Pellets Process.. |
|||
Melt Flow | 11.0 - 26.0 g/10 min | 11.0 - 26.0 g/10 min | Average value: 17.7 g/10 min Grade Count:3 |
Overview of materials for ABS/Polyurethane Alloy This property data is a summary of similar materials in the MatWeb database for the category "ABS/Polyurethane Alloy". Each property range of values reported is minimum and maximum values of appropr.. |