Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Techmer ES HiFill® PA4/6 GF30 HS NAT 30% Glass Filled (Conditioned)

Category Polymer , Thermoplastic , Nylon , Nylon 46 , Nylon 46, Glass Fiber Reinforced
Manufacturer Techmer ES
Trade Name HiFill®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Techmer ES HiFill® PA4/6 GF30 HS NAT 30% Glass Filled (Conditioned).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 30% Filler by WeightAdditive: Heat StabilizerFeatures: Heat StabilizedAppearance: Natural ColorInformation provided by TP Composites, Inc.
Physical Properties Metric English Comments
Density 1.41 g/cc
0.0509 lb/in³
ASTM D792
Water Absorption 1.5 %

@Time 86400 sec
1.5 %

@Time 24.0 hour
ASTM D570
Linear Mold Shrinkage, Flow 0.0060 cm/cm

@Thickness 3.17 mm
0.0060 in/in

@Thickness 0.125 in
ASTM D955
Mechanical Properties Metric English Comments
Tensile Strength, Yield 117 MPa
17000 psi
ASTM D638
Elongation at Yield 7.0 %
7.0 %
ASTM D638
Flexural Yield Strength 186 MPa
27000 psi
ASTM D790
Flexural Modulus 5.38 GPa
780 ksi
ASTM D790
Izod Impact, Notched 1.49 J/cm

@Thickness 3.17 mm
2.80 ft-lb/in

@Thickness 0.125 in
ASTM D256