Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 5.38 GPa | 780 ksi | ASTM D790 |
Polymer Resources PPX/NY G20 PPO/Nylon 66 Alloy , 20% Glass Reinforced Polyphenylene Oxide/Nylon 66 Alloy , 20% Glass ReinforcedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Informa.. |
|||
Flexural Modulus | 5.38 GPa @Thickness 3.17 mm |
780 ksi @Thickness 0.125 in |
ASTM D790 |
PTS Tristar® PC-20GF 20% Glass Reinforced Polycarbonate Information provided by Polymer Technology and Services, LLC (PTS). |
|||
Flexural Modulus | 5.38 GPa @Temperature 150 °C |
780 ksi @Temperature 302 °F |
ISO 178 |
Solvay Specialty Polymers Amodel® A-1145 HS Polyphthalamide (PPA)
(Unverified Data**) Amodel A-1145 HS is a 45% glass reinforced, heat stabilized polyphthalamide (PPA) with a high heat deflection temperature, very high flexural modulus and very high tensile strength. Excellent creep .. |
|||
Flexural Modulus | 5.38 GPa | 780 ksi | ASTM D790 |
Polymer Resources PPX/NY G20 Modified PPO, 20% Glass Reinforced PPX/Nylon 6,6 Alloy
(Unverified Data**)&l Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Information provided by Polymer Resources Corporation. |
|||
Flexural Modulus | 5.38 GPa @Thickness 3.17 mm |
780 ksi @Thickness 0.125 in |
ASTM D790 |
PTS Tristar® PC-20GFR 20% Glass Reinforced Polycarbonate With Release Information provided by Polymer Technology and Services, LLC (PTS). |
|||
Flexural Modulus | 5.38 GPa | 780 ksi | initial |
Malvern Minerals Thermoplastic Polyester with Novacite® 1250 Quartz Filler Product data demonstrates the effect of the Novacite (untreated lamellar quartz) filler. A separate entry demonstrates the effect of surface-treated Novakup filler in thermoplastic polyester Th.. |
|||
Flexural Modulus | 5.38 GPa | 780 ksi | ASTM D790 |
Global GPP-130-C 30% Glass Filled Chemically Coupled Polypropylene Information provided by Global Polymers Corporation. |
|||
Flexural Modulus | 5.38 GPa @Temperature 150 °C |
780 ksi @Temperature 302 °F |
ISO 178 |
Solvay Specialty Polymers Amodel® A-1145 HS Polyphthalamide (PPA), 45% Glass Fiber (Dry) Amodel® A-1145 HS is a 45% glass reinforced, heat stabilized polyphthalamide (PPA) with a high heat deflection temperature, very high flexural modulus and very high tensile strength. Excellent cr.. |
|||
Flexural Modulus | 5.38 GPa | 780 ksi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics Valox® V8030CS PBT+PET Glass filled Valox with enhanced surface |
|||
Flexural Modulus | 5.38 GPa | 780 ksi | ASTM D790 |
Techmer ES HiFill® PA4/6 GF30 HS NAT 30% Glass Filled (Conditioned) Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 30% Filler by WeightAdditive: Heat StabilizerFeatures: Heat StabilizedAppearance: Natural ColorInformation p.. |
|||
Flexural Modulus | 5.38 GPa | 780 ksi | ASTM D790 |
Techmer ES HiFill® PA4/6 GF33 HS NAT 33% Glass Filled (Conditioned) Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 33% Filler by WeightAdditive: Heat StabilizerFeatures: Heat StabilizedAppearance: Natural ColorInformation p.. |
|||
Flexural Modulus | 5.38 GPa | 780 ksi | Tangent; ASTM D790 |
Plastics Group Polifil® GFPC-20 20% Glass-Reinforced Polycarbonate Polifil® GFPC series compounds offer a combination of improved dimensional stability and decreased flammability. The excellent balance of physical properties make the Polifil® glass-filled polycar.. |
|||
Flexural Modulus | 5.38 GPa | 780 ksi | ASTM D790 |
Chase Plastics CP Pryme® PC120R Polycarbonate, 20% Glass Fiber Reinforced Features: Good mold releaseForm: PelletsInformation provided by Chase Plastics. |
|||
Flexural Modulus | 5.38 GPa | 780 ksi | ASTM D790 |
Ensinger Tecapeek® XP-105 Compression Molded PEEK Compound, 15% Graphite Filled Ensinger Special Polymers offers over twenty different VICTREX® PEEK blends to choose from and has the capability to blend custom compounds for specific applications. Compression molding results in.. |
|||
Flexural Modulus | 5.38 GPa | 780 ksi | ASTM D790 |
Asahi Kasei Thermylene® P6-30FG-0602 30% Glass Fiber Reinforced, UV Stabilized Information provided by Asahi Thermofil |
|||
Flexural Modulus | 5.38 GPa | 780 ksi | ASTM D790 |
PolyOne Edgetek® ATH-30GF/000 Acetal-Homopolymer, Glass Filled
(discontinued **) Description/Features:Glass Fiber ReinforcedUL 94 HBPolyOne First ChoiceInformation provided by PolyOne Corporation. |
|||
Flexural Modulus | 5.38 GPa | 780 ksi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics LNP THERMOCOMP AX06472 ABS LNP* Thermocomp* AX06472 is a compound based on ABS containing a clay blend. |