Mechanical Properties Metric English Comments
Flexural Modulus 5.38 GPa
780 ksi
ASTM D790
Polymer Resources PPX/NY G20 PPO/Nylon 66 Alloy , 20% Glass Reinforced
Polyphenylene Oxide/Nylon 66 Alloy , 20% Glass ReinforcedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Informa..
Flexural Modulus 5.38 GPa

@Thickness 3.17 mm
780 ksi

@Thickness 0.125 in
ASTM D790
PTS Tristar® PC-20GF 20% Glass Reinforced Polycarbonate
Information provided by Polymer Technology and Services, LLC (PTS).
Flexural Modulus 5.38 GPa

@Temperature 150 °C
780 ksi

@Temperature 302 °F
ISO 178
Solvay Specialty Polymers Amodel® A-1145 HS Polyphthalamide (PPA)  (Unverified Data**)
Amodel A-1145 HS is a 45% glass reinforced, heat stabilized polyphthalamide (PPA) with a high heat deflection temperature, very high flexural modulus and very high tensile strength. Excellent creep ..
Flexural Modulus 5.38 GPa
780 ksi
ASTM D790
Polymer Resources PPX/NY G20 Modified PPO, 20% Glass Reinforced PPX/Nylon 6,6 Alloy  (Unverified Data**)&l
Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Information provided by Polymer Resources Corporation.
Flexural Modulus 5.38 GPa

@Thickness 3.17 mm
780 ksi

@Thickness 0.125 in
ASTM D790
PTS Tristar® PC-20GFR 20% Glass Reinforced Polycarbonate With Release
Information provided by Polymer Technology and Services, LLC (PTS).
Flexural Modulus 5.38 GPa
780 ksi
initial
Malvern Minerals Thermoplastic Polyester with Novacite® 1250 Quartz Filler
Product data demonstrates the effect of the Novacite (untreated lamellar quartz) filler. A separate entry demonstrates the effect of surface-treated Novakup filler in thermoplastic polyester Th..
Flexural Modulus 5.38 GPa
780 ksi
ASTM D790
Global GPP-130-C 30% Glass Filled Chemically Coupled Polypropylene
Information provided by Global Polymers Corporation.
Flexural Modulus 5.38 GPa

@Temperature 150 °C
780 ksi

@Temperature 302 °F
ISO 178
Solvay Specialty Polymers Amodel® A-1145 HS Polyphthalamide (PPA), 45% Glass Fiber (Dry)
Amodel® A-1145 HS is a 45% glass reinforced, heat stabilized polyphthalamide (PPA) with a high heat deflection temperature, very high flexural modulus and very high tensile strength. Excellent cr..
Flexural Modulus 5.38 GPa
780 ksi
1.3 mm/min, 50 mm span; ASTM D790
SABIC Innovative Plastics Valox® V8030CS PBT+PET
Glass filled Valox with enhanced surface
Flexural Modulus 5.38 GPa
780 ksi
ASTM D790
Techmer ES HiFill® PA4/6 GF30 HS NAT 30% Glass Filled (Conditioned)
Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 30% Filler by WeightAdditive: Heat StabilizerFeatures: Heat StabilizedAppearance: Natural ColorInformation p..
Flexural Modulus 5.38 GPa
780 ksi
ASTM D790
Techmer ES HiFill® PA4/6 GF33 HS NAT 33% Glass Filled (Conditioned)
Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 33% Filler by WeightAdditive: Heat StabilizerFeatures: Heat StabilizedAppearance: Natural ColorInformation p..
Flexural Modulus 5.38 GPa
780 ksi
Tangent; ASTM D790
Plastics Group Polifil® GFPC-20 20% Glass-Reinforced Polycarbonate
Polifil® GFPC series compounds offer a combination of improved dimensional stability and decreased flammability. The excellent balance of physical properties make the Polifil® glass-filled polycar..
Flexural Modulus 5.38 GPa
781 ksi
ASTM D790
PlastxWorld CEVIAN®-N GRSJ1 10% GF SAN resin
Glass fiber reinforced SAN resin. These are typical values and are not intended for specification purposes. UL approved file No. is E47773. Information provided by PlastxWorld Inc.
Flexural Modulus 5.38 GPa
780 ksi
ASTM D790
Chase Plastics CP Pryme® PC120R Polycarbonate, 20% Glass Fiber Reinforced
Features: Good mold releaseForm: PelletsInformation provided by Chase Plastics.
Flexural Modulus 5.38 GPa
780 ksi
ASTM D790
Ensinger Tecapeek® XP-105 Compression Molded PEEK Compound, 15% Graphite Filled
Ensinger Special Polymers offers over twenty different VICTREX® PEEK blends to choose from and has the capability to blend custom compounds for specific applications. Compression molding results in..
Flexural Modulus 5.38 GPa
780 ksi
ASTM D790
Asahi Kasei Thermylene® P6-30FG-0602 30% Glass Fiber Reinforced, UV Stabilized
Information provided by Asahi Thermofil
Flexural Modulus 5.38 GPa
780 ksi
ASTM D790
PolyOne Edgetek® ATH-30GF/000 Acetal-Homopolymer, Glass Filled  (discontinued **)
Description/Features:Glass Fiber ReinforcedUL 94 HBPolyOne First ChoiceInformation provided by PolyOne Corporation.
Flexural Modulus 5.38 GPa
780 ksi
1.3 mm/min, 50 mm span; ASTM D790
SABIC Innovative Plastics LNP THERMOCOMP AX06472 ABS
LNP* Thermocomp* AX06472 is a compound based on ABS containing a clay blend.