Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 117 MPa | 17000 psi | ASTM D638 |
PolyOne LubriOne™ NN-30GF/13T-2S Black Polyamide 66 (Nylon 66) LubriOne™ Lubricated and Wear-Resistant Compounds have been specifically formulated to be self-lubricating materials, offering low coefficient of friction and improved wear resistance properties. L.. |
|||
Tensile Strength, Yield | 117 MPa | 17000 psi | Type I, 5.1 mm/min; ASTM D638 |
PolyOne Nymax™ GMF 604 40 UV Black 115 1 X 1 Polyamide 6 (Nylon 6) The Nymax® GMF 600 Series of compounds are based upon nylon 6 resins and select combinations of glass fiber and mineral reinforcements offering a unique balance of physical property and part perfor.. |
|||
Tensile Strength, Yield | 117 MPa | 17000 psi | ASTM D638 |
Polymer Resources PPX-FRG30 Modified-PPO, V-1 Flame Retardant, 30% Glass Reinforced Modified-Polyphenylene Oxide, V-1 Flame Retardant, 30% Glass ReinforcedFeatures: • Bromine Free • Chlorine FreeProcess: Injection MoldingNotes: All physical, mechanical and thermal testing condu.. |
|||
Tensile Strength, Yield | 117 MPa | 17000 psi | ASTM D638 |
Polymer Resources TP-G30 Polybutylene Terephthalate, 30% Glass Reinforced Polybutylene Terephthalate, 30% Glass ReinforcedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information prov.. |
|||
Tensile Strength, Yield | 117 MPa | 17000 psi | ASTM D638 |
Polymer Resources TPSF-G30 Polybutylene Terephthalate, Structural Foam, 30% Glass Reinforced Polybutylene Terephthalate, Structural Foam, 30% Glass Reinforced Process: Foam MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Inf.. |
|||
Tensile Strength, Yield | 117 MPa | 17000 psi | ASTM D638 |
Custom Resins Vexel™ 4200 RD PBT; 30% GF, FR
(discontinued **) Property data for dry as molded samples.Data provided by the manufacturer |
|||
Tensile Strength, Yield | 117 MPa @Temperature 23.0 °C |
17000 psi @Temperature 73.4 °F |
ISO 527 |
DuPont Performance Polymers Crastin® CE15330 BK010 PBT
(Unverified Data**) Crastin® CE15330 BK010 is a 30% glass reinforced flame retardant polybutylene terephthalate molding resin. It is recognized as UL94 V-0 at 0.71mm(0.028in).Information provided by DuPont Performance.. |
|||
Tensile Strength, Yield | 117 MPa | 17000 psi | Type I, 5 mm/min; ASTM D638 |
LNP NORYL® EXCP0112 PPS + Polyphenylene Ether, 40% Glass / Mineral Reinforcement
(discontinued **) For applications requiring voltage resistance.Features: Corona resistantForms: PelletsProcessing Method: Injection MoldingInformation provided by LNP, a GE Plastics Company.This data sheet is labele.. |
|||
Tensile Strength, Yield | 117 MPa | 17000 psi | ASTM D638 |
PolyOne Edgetek® SF-40GF-25MN1/000 PPS (Polyphenylene Sulfide), 40% Glass Fiber and 25% Mineral Filled
(disco Information provided by PolyOne™ Corporation |
|||
Tensile Strength, Yield | 117 MPa | 17000 psi | ASTM D638 |
LG Chemical Lupox® PBT-LW5303 30% Glass Filled Low Warp PBT Low Warpage. Information provided by US distributor Polymer Technology and Services, LLC (PTS). |
|||
Tensile Strength, Yield | 117 MPa | 17000 psi | ASTM D638 |
Techmer ES Elastoblend® PBT GF33 IM 33% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 33% Filler by WeightAdditive: Impact ModifierFeatures: Impact ModifiedInformation provided by TP Composites,.. |
|||
Tensile Strength, Yield | 117 MPa | 17000 psi | Type I, 5 mm/min; ASTM D638 |
SABIC Innovative Plastics ULTEM CRS5111 PEI 10% Glass fiber filled, enhanced flow Polyetherimide copolymer (Tg 225C) with enhanced chemical resistance to strong acids, bases, aromatics, and ketones. ECO conforming, UL94 V0 and 5 VA listing. |
|||
Tensile Strength, Yield | 117 MPa | 17000 psi | 5 mm/min; ISO 527 |
SABIC Innovative Plastics LNP STAT-KON DE0026E PC (Europe-Africa-Middle East) LNP* Stat-kon* DE0026E is a compound based on Polycarbonate resin containing Flame Retardant, Carbon Fiber. Added features of this material include: Electrically Conductive, Flame Retardant. |
|||
Tensile Strength, Yield | 117 MPa | 17000 psi | ASTM D638 |
Techmer ES HiFill® ABS GF60 LE 60% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 60% Filler by WeightFeatures: Low ExtractablesInformation provided by TP Composites, Inc. |
|||
Tensile Strength, Yield | 117 MPa | 17000 psi | SABIC - Japan Method |
SABIC Innovative Plastics Valox® AB9530 ABS+PBT (Asia Pacific) This data was supplied by SABIC-IP for the Asia Pacific region. |
|||
Tensile Strength, Yield | 117 MPa | 17000 psi | 5 mm/min; ISO 527 |
SABIC Innovative Plastics Valox® SHF436HR PBT PBT, Super High Flow, 30% glass reinforced,hydrolytically resistant. |
|||
Tensile Strength, Yield | 117 MPa | 17000 psi | Type I, 5 mm/min; ASTM D638 |
SABIC Innovative Plastics LNP STAT-KON Noryl_NC3508 PPE+HIPS (Europe-Africa-Middle East) PRELIMINARY DATA. LNP* Stat-kon* Noryl_NC3508 compound is a 33% glass/mineral/carbon filled PPE+PS. ESD, high heat, tight tolerance: electronic packaging/chip trays. |
|||
Tensile Strength, Yield | 117 MPa | 17000 psi | 5 mm/min; ISO 527 |
SABIC Innovative Plastics LNP THERMOCOMP DF004 PC (Europe-Africa-Middle East) LNP* THERMOCOMP* DF004 is a compound based on Polycarbonate resin containing Glass Fiber. |
|||
Tensile Strength, Yield | 117 MPa | 17000 psi | ASTM D638 |
Techmer ES Plastiblend® TPX-HTN-000CB 15% Glass Filled Availability: North AmericaForms: Pellets Filler/Reinforcement: Glass Fiber Reinforcement, 15% Filler by WeightFeatures: High Heat ResistanceInformation provided by TP Composites, Inc. |
|||
Tensile Strength, Yield | 117 MPa | 17000 psi | SABIC - Japan Method |
SABIC Innovative Plastics Noryl GTX GTX870 PPE+PA6 (Asia Pacific) This data was supplied by SABIC-IP for the Asia Pacific region. |
|||
Tensile Strength, Yield | 117 MPa | 17000 psi | ASTM D 638 |
SABIC Innovative Plastics LNP Lubricomp KCL36 Acetal Copoly LNP* Lubricomp* KCL36 is a compound based on Acetal Copolymer resin containing PTFE, Carbon Fiber. Added features of this material include: Internally Lubricated, Electrically Conductive.This data .. |
|||
Tensile Strength, Yield | 117 MPa | 17000 psi | Type I, 5 mm/min; ASTM D 638 |
SABIC Innovative Plastics Ultem ATX102R PEI+PCE 20% Glass fiber filled, high flow Polyetherimide blend with internal mold release. ECO Conforming, UL94 V0 and 5VA listing.This data was supplied by SABIC-IP for the Americas region. |
|||
Tensile Strength, Yield | 117 MPa | 17000 psi | ASTM D638 |
Techmer ES Electrablend® PA6 GF20 20% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 20% Filler by Weight/Unspecified Filler/Reinfor.Additive: LubricantFeatures: Conductive and LubricatedAppear.. |
|||
Tensile Strength, Yield | 117 MPa | 17000 psi | Type I, 5 mm/min; ASTM D638 |
SABIC Innovative Plastics Valox® IQNH4565 PBT (Asia Pacific) Valox* iQNH4565 resin is a non-brominated/non-chlorinated flame retardant product based on an environmentally sustainable Valox iQ* PBT resin. Post-consumer recycle (PCR) usage is 29% based on EPEAT.. |
|||
Tensile Strength, Yield | 117 MPa | 17000 psi | ASTM D638 |
Techmer ES HiFill® PA4/6 GF30 HS NAT 30% Glass Filled (Conditioned) Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 30% Filler by WeightAdditive: Heat StabilizerFeatures: Heat StabilizedAppearance: Natural ColorInformation p.. |
|||
Tensile Strength, Yield | 117 MPa | 17000 psi | ASTM D638 |
Clariant PA123G25 Nylon 66, 25% Glass Fiber, Impact Modified, Heat Stabilized Data provided by Clariant Masterbatches |
|||
Tensile Strength, Yield | 117 MPa @Temperature -40.0 °C |
17000 psi @Temperature -40.0 °F |
ISO Data |
BASF Ultramid® 8253 PA6 (Dry) Ultramid 8253 is an unfilled, impact modified type 6 graft copolymer developed for both injection molding and extrusion applications. It is also available in heat stabilized (Ultramid 8253 HS) and/o.. |
|||
Tensile Strength, Yield | 117 MPa | 17000 psi | ISO 527-2 |
Ascend Performance Materials Vydyne® R525 Nylon 66, 25% Glass Reinforced, Conditioned Vydyne® R525 is hydrolysis-resistant, 25% glass-fiber reinforced PA66 resin. Available in natural it is lubricated for improved machine feed and flow. Glass-reinforced Vydyne resins provide higher .. |
|||
Tensile Strength, Yield | 117 MPa | 17000 psi | ASTM D638 |
Techmer ES Electrablend® ABS CF40 BK 40% Carbon Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Carbon Fiber, 40% Filler by WeightAppearance: BlackInformation provided by TP Composites, Inc. |