Techmer ES HiFill® PA12 GF30 HS L 30% Glass Filled

Category Polymer , Thermoplastic , Nylon , Nylon 12 , Nylon 12, 30% Glass Fiber Filled
Manufacturer Techmer ES
Trade Name HiFill®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Techmer ES HiFill® PA12 GF30 HS L 30% Glass Filled.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 30% Filler by WeightAdditive: Heat Stabilizer and LubricantFeatures: Heat Stabilized and LubricatedInformation provided by TP Composites, Inc.
Physical Properties Metric English Comments
Density 1.24 g/cc
0.0448 lb/in³
ASTM D792
Water Absorption 0.12 %

@Time 86400 sec
0.12 %

@Time 24.0 hour
ASTM D570
Linear Mold Shrinkage, Flow 0.0040 cm/cm

@Thickness 3.17 mm
0.0040 in/in

@Thickness 0.125 in
ASTM D955
Mechanical Properties Metric English Comments
Tensile Strength, Yield 108 MPa
15600 psi
ASTM D638
Elongation at Break 3.0 %
3.0 %
ASTM D638
Flexural Strength 150 MPa
21700 psi
ASTM D790
Flexural Modulus 5.52 GPa
800 ksi
ASTM D790
Izod Impact, Notched 1.55 J/cm

@Thickness 3.17 mm
2.90 ft-lb/in

@Thickness 0.125 in
ASTM D256
Izod Impact, Unnotched NB
NB
ASTM D256
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 41.4 µm/m-°C
23.0 µin/in-°F
ASTM D696
Deflection Temperature at 0.46 MPa (66 psi) 138 °C
280 °F
Unannealed; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 160 °C
320 °F
Unannealed; ASTM D648
Electrical Properties Metric English Comments
Dielectric Strength 17.7 kV/mm
450 kV/in
Method A (Short-Time); ASTM D149