Sylvin Technologies 9600-95 Clear PVC Molding Compound

Category Polymer , Thermoplastic , Vinyl (PVC) , PVC, Molded
Manufacturer Sylvin Technologies
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Sylvin Technologies 9600-95 Clear PVC Molding Compound.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Information provided by Sylvin Technologies Inc.
Physical Properties Metric English Comments
Specific Gravity 1.28 g/cc
1.28 g/cc
Mechanical Properties Metric English Comments
Hardness, Shore A 95
95
10 seconds
Tensile Strength, Ultimate 18.6 MPa
2700 psi
Elongation at Break 240 %
240 %
Tear Strength Test 530
530
Optical Properties Metric English Comments
Transmission, Visible 90 %
90 %
clear; thickness not quantified
Processing Properties Metric English Comments
Melt Temperature 174 - 185 °C
345 - 365 °F