Processing Properties | Metric | English | Comments |
---|---|---|---|
Melt Temperature | 179 - 185 °C | 354 - 365 °F | |
PolyOne Geon™ Vinyl Flexible A5D00 Polyvinyl Chloride, Flexible (PVC, Flexible) Recommended for interior applications.Information provided by PolyOne |
|||
Melt Temperature | 179 - 185 °C | 354 - 365 °F | |
PolyOne Geon™ Vinyl Flexible A5DM0 Polyvinyl Chloride, Flexible (PVC, Flexible) Recommended for interior applications.Information provided by PolyOne |
|||
Melt Temperature | 179 - 185 °C | 354 - 365 °F | |
PolyOne Geon™ Vinyl Flexible B5DU0 Polyvinyl Chloride, Flexible (PVC, Flexible) Information provided by PolyOne |
|||
Melt Temperature | 179 - 185 °C | 354 - 365 °F | |
PolyOne Geon™ Vinyl Flexible B6D00 Polyvinyl Chloride, Flexible (PVC, Flexible) Information provided by PolyOne |
|||
Melt Temperature | 179 - 185 °C | 354 - 365 °F | |
PolyOne Geon™ Vinyl Flexible B8501 Polyvinyl Chloride, Flexible (PVC, Flexible) A flexible Vinyl compound for hose and tubing applications with enhanced physical characteristics.Information provided by PolyOne |
|||
Melt Temperature | 174 - 185 °C | 345 - 365 °F | |
PolyOne Geon™ Vinyl Flexible B9WF1 Polyvinyl Chloride, Flexible (PVC, Flexible) Information provided by PolyOne |
|||
Melt Temperature | 179 - 185 °C | 354 - 365 °F | |
PolyOne Geon™ Vinyl Flexible C5D00 Polyvinyl Chloride, Flexible (PVC, Flexible) Information provided by PolyOne |
|||
Melt Temperature | 179 - 185 °C | 354 - 365 °F | |
PolyOne Geon™ Vinyl Flexible F77E Polyvinyl Chloride, Flexible (PVC, Flexible) Information provided by PolyOne |
|||
Melt Temperature | 179 - 185 °C | 354 - 365 °F | |
PolyOne Geon™ Vinyl Flexible MG23B Polyvinyl Chloride, Flexible (PVC, Flexible) Information provided by PolyOne |
|||
Melt Temperature | 177 - 185 °C | 351 - 365 °F | |
PolyOne Geon™ Vinyl Flexible P502 Polyvinyl Chloride, Flexible (PVC, Flexible) Information provided by PolyOne |
|||
Melt Temperature | 179 - 185 °C | 354 - 365 °F | |
PolyOne Geon™ Vinyl Flexible R340AE Polyvinyl Chloride, Flexible (PVC, Flexible) Information provided by PolyOne |
|||
Melt Temperature | 179 - 185 °C | 354 - 365 °F | |
PolyOne Geon™ Vinyl Flexible B5D01 Polyvinyl Chloride, Flexible (PVC, Flexible) Information provided by PolyOne |
|||
Melt Temperature | 179 - 185 °C | 354 - 365 °F | |
PolyOne Geon™ Vinyl Flexible B5DG1 Polyvinyl Chloride, Flexible (PVC, Flexible) Information provided by PolyOne |
|||
Melt Temperature | 179 - 185 °C | 354 - 365 °F | |
PolyOne Geon™ Vinyl Flexible G92B Polyvinyl Chloride, Flexible (PVC, Flexible) Information provided by PolyOne |
|||
Melt Temperature | 177 - 185 °C | 351 - 365 °F | |
PolyOne Geon™ Vinyl Flexible R264AE Polyvinyl Chloride, Flexible (PVC, Flexible) Information provided by PolyOne |
|||
Melt Temperature | 179 - 185 °C | 354 - 365 °F | |
PolyOne Geon™ Vinyl Flexible R267AM Polyvinyl Chloride, Flexible (PVC, Flexible) Information provided by PolyOne |
|||
Melt Temperature | 179 - 185 °C | 354 - 365 °F | |
PolyOne Geon™ Vinyl Flexible R279AE Polyvinyl Chloride, Flexible (PVC, Flexible) Information provided by PolyOne |
|||
Melt Temperature | 174 - 185 °C | 345 - 365 °F | |
Huntsman PE 1302 EVA Film Extrusion
(discontinued **) 3% Vinyl Acetate EVA copolymer and FDA compliantFeatures: High clarity film with good low temperature toughness and heat seal characteristics.Applications: Film extrusion: food packaging, general pu.. |
|||
Melt Temperature | 174 - 185 °C | 345 - 365 °F | |
Sylvin Technologies 8960-95 Natural PVC Extrusion Compound Information provided by Sylvin Technologies Inc. |
|||
Melt Temperature | 174 - 185 °C | 345 - 365 °F | |
Sylvin Technologies 9077-95 LMW Natural PVC for Injection Molding Information provided by Sylvin Technologies Inc. |
|||
Melt Temperature | 174 - 185 °C | 345 - 365 °F | |
Sylvin Technologies 916V0-95 Natural PVC for Injection Molding Information provided by Sylvin Technologies Inc. |
|||
Melt Temperature | 174 - 185 °C | 345 - 365 °F | |
Sylvin Technologies 9925-95 Natural PVC Molding Compound Information provided by Sylvin Technologies Inc. |
|||
Melt Temperature | 174 - 185 °C | 345 - 365 °F | |
Sylvin Technologies 9940-95 Natural PVC Molding Compound Information provided by Sylvin Technologies Inc. |
|||
Melt Temperature | 174 - 185 °C | 345 - 365 °F | |
Sylvin Technologies 9950-95 Natural PVC Molding Compound Information provided by Sylvin Technologies Inc. |
|||
Melt Temperature | 174 - 185 °C | 345 - 365 °F | |
Sylvin Technologies 9960-95 Natural PVC Molding Compound Information provided by Sylvin Technologies Inc. |
|||
Melt Temperature | 174 - 185 °C | 345 - 365 °F | |
Sylvin Technologies 9999-95 Natural PVC Molding Compound Information provided by Sylvin Technologies Inc. |
|||
Melt Temperature | 160 - 185 °C | 320 - 365 °F | Blown Film Coextrusion |
DuPont™ Appeel® 72D727 Sealing Resin DuPont™ Appeel® 72D727 is a blown or cast film resin designed to be a sealing layer to film or sheet lidding applications. It provides a peelable seal to a number of materials including HDPE, LLDP.. |
|||
Melt Temperature | 160 - 185 °C | 320 - 365 °F | Blown Film Coextrusion |
DuPont™ Appeel® 20D784 Ethylene Acrylate Appeel® 20D784 is a modified ethylene acrylate resin designed to function as a sealing layer for lidding applications. It is most often suggested to provide peelable seals over a broad temperature .. |
|||
Melt Temperature | 125 - 185 °C | 257 - 365 °F | |
Borealis LE7704 Polyethylene Compound, Semiconductive, Thermoplastic LE7704 is a thermoplastic black polyethylene compound, specially designed for semiconductive screen applications. Applications: LE7704 is intended for semiconductive applications in medium voltage.. |
|||
Melt Temperature | 174 - 185 °C | 345 - 365 °F | |
Huntsman PE 1375 EVA Film Extrusion
(discontinued **) 3.7% Vinyl Acetate EVA copolymer and FDA compliantFeatures: Excellent balance of optical and strength, toughness and flexibility at low temperatures, and good heat seal characteristic.Applications: .. |