Material Notes:
Key Features: medium melt flow, medium modulus thermoplastic elastomeric olefin resin, good impact and stiffness balance, good dimensional stability, good processabilityApplications: molded-in color automotive bumper step pads, rub strips, sight shields, scuff platesDescription: Hifax ETA-3104HF, medium melt flow, thermoplastic elastomeric olefin resin has a very good combination of properties and prcessability. It was designed for a varity of molded-in color automotive exterior components and is available in UV-stabilized form for that purpose.Information provided by Montell Polyolefins.LyondellBasell is the successor company to Montell.
Physical Properties Metric English Comments
Density 0.900 g/cc
0.0325 lb/in³
ISO 1183
Linear Mold Shrinkage 0.011 cm/cm
0.011 in/in
Tool, Montell
Melt Flow 9.0 g/10 min

@Load 2.16 kg,
Temperature 230 °C
9.0 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Shore D 57
57
ISO 686
Tensile Strength, Yield 14.0 MPa
2030 psi
ISO R527-1
Elongation at Yield 10 %
10 %
ISO R527-1
Flexural Modulus 0.550 GPa
79.8 ksi
ISO 178
Izod Impact, Notched 0.520 J/cm

@Temperature -40.0 °C
0.974 ft-lb/in

@Temperature -40.0 °F
ISO 180
Thermal Properties Metric English Comments
CTE, linear 96.0 µm/m-°C

@Temperature -30.0 - 100 °C
53.3 µin/in-°F

@Temperature -22.0 - 212 °F
ASTM D696
Deflection Temperature at 0.46 MPa (66 psi) 66.0 °C
151 °F
ISO 75
Deflection Temperature at 1.8 MPa (264 psi) 43.0 °C
109 °F
ISO 75