Material Notes:
Lower cost Hy-Bor version. Combining Specialty Materials' boron fiber with graphite prepreg, Hy-Bor® is a high-performance material with exceptional properties. Available with 4.0 and 5.6 mil boron fibers, Hy-Bor material can be manufactured to incorporate any commercially available graphite prepreg. By altering the spacing of the boron fiber in the prepreg, performance properties and material costs can be tailored to meet the needs of a variety of demanding applications.Information provided by Specialty Materials, Inc.
Physical Properties Metric English Comments
Density 1.82 g/cc
0.0658 lb/in³
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 1620 MPa
235000 psi
Elongation at Yield 0.80 %
0.80 %
Modulus of Elasticity 207 GPa
30000 ksi
Flexural Yield Strength 2275 MPa
330000 psi
Flexural Modulus 207 GPa
30000 ksi
Compressive Yield Strength 2344 MPa
340000 psi
Compressive Modulus 193 GPa
28000 ksi
Shear Strength 103 MPa
14900 psi
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 177 °C
351 °F
Processing Properties Metric English Comments
Processing Temperature 121 °C
250 °F
Users viewing this material also viewed the following: