Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Shear Strength 103 MPa
15000 psi
ASTM D732
Quadrant EPP Duratron® PEI U1000 LSG Polyetherimide, unfilled, extruded, Biocompatibility tested (ASTM Product Data Sheet)
Duratron® U1000 (Formerly Ultem® 1000) polyetherimide is an amorphous, high-performance polymer with exceptional flame and heat resistance. It performs continuously to 340°F (171°C), making it..
Shear Strength 103 MPa
15000 psi
ASTM D732
Quantum PEI - Ultem®
Information provided by Quantum Advanced Engineering Plastics
Shear Strength 103 MPa
14900 psi
ASTM D732
Solvay Specialty Polymers KetaSpire® KT-880 CF30 Polyetheretherketone (PEEK)  (Unverified Data**)
KetaSpire KT-880 CF30 is a high flow, 30% carbon fiber reinforced grade of polyetheretherketone (PEEK). Carbon-fiber reinforcement of KetaSpire PEEK provides the maximum levels of mechanical propert..
Shear Strength 103 MPa
15000 psi
ASTM D732
Quadrant EPP Duratron® PEI U1000 Extruded Unfilled Polyetherimide (ASTM Product Data Sheet)
Shear Strength 103 MPa
15000 psi
XP Phenolic Laminate
Paper based phenolic provides low cost electrical and mechanical properties. It is widely used for switchboards, panel boards, insulating washers, and intricate punched parts.Information provided b..
Shear Strength 103 MPa
15000 psi
Solvay Specialty Polymers Ryton® R-4 Polyphenylene Sulfide Compound  (Unverified Data**)
Natural Color Polyphenylene Sulfide CompoundRyton® R-4 is a 40% fiberglass reinforced polyphenylene sulfide compound which provides outstanding chemical resistance and mechanical properties even at..
Shear Strength 103 MPa

@Thickness 15.7 mm
15000 psi

@Thickness 0.620 in
ASTM D732
Industrial Laminates/Norplex NP610 Paper Base Laminate
Description: Phenolic paper based grade for mechanical applications. Good tensile, compressive and flexural strength. Primarily a machining material, but may be hot punched up to .093" thick.Thickne..
Shear Strength 103 MPa
14900 psi
ASTM D732
Haysite H258 Polyester Laminate
Solder Pallet and Work Holder Sheet A high temperature polyester laminate that exhibits excellent retention of mechanical properties and dimensional stability at elevated temperatures. Applications..
Shear Strength 103 MPa
14900 psi
ASTM D732
Haysite H260 Polyester Laminate
Solder Pallet and Work Holder Sheet An advanced composite that is high temperature resistant and high strength with semi-conductive properties. Engineered for use as wave and reflow solder pallet m..
Shear Strength 103 MPa
14900 psi
ASTM D732
Haysite H755 Glass Reinforced Polyester Sheet, Electrical Grade (GPO1)
A new generation of IEEE Class F, 155ºC /165ºC NEMA GPO- 1 material. H755 is designed to bridge the gap between 130ºC Class B GPO-1 materials and Class H 180ºC grades. H755 has quickly g..
Shear Strength 103 MPa
14900 psi
ASTM D732
Solvay Specialty Polymers KetaSpire® KT-880 CF30 Polyetheretherketone (PEEK), 30% Carbon Fiber
KetaSpire® KT-880 CF30 is a high flow, 30% carbon fiber reinforced grade of polyetheretherketone (PEEK). Carbon-fiber reinforcement of KetaSpire® PEEK provides the maximum levels of mechanical..
Shear Strength 103 MPa
14900 psi
Specialty Materials Hy-Bor 100 Boron/Graphite Hybrid Prepreg Tape
Lower cost Hy-Bor version. Combining Specialty Materials' boron fiber with graphite prepreg, Hy-Bor® is a high-performance material with exceptional properties. Available with 4.0 and 5.6 m..
Shear Strength 103 MPa
14900 psi
Specialty Materials Hy-Bor Boron/Graphite Hybrid Prepreg Tape
Boron & Graphite prepreg. Combining Specialty Materials' boron fiber with graphite prepreg, Hy-Bor® is a high-performance material with exceptional properties. Available with 4.0 and 5.6 mil..
Shear Strength 103 MPa
15000 psi
Ultimate
Ensinger TECAPEI® made from Ultem® 1000 PEI
TECAPEI™ is an amorphous thermoplastic polyetherimide (PEI) made from Sabic Innovative Plastics' Ultem® 1000 and 2000 series resins. The unreinforced 1000 series materials are translucent amber in..
Shear Strength 103 MPa
15000 psi
ASTM D732
PolyOne Edgetek® PI-40GF/000 Polyetherimide (PEI), Glass Filled  (discontinued **)
Description/Features:Glass Fiber ReinforcedUL 94 V0PolyOne First ChoiceInformation provided by PolyOne Corporation.