Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Ultimate | 1620 MPa | 235000 psi | 282°C Temper Temperature |
Latrobe Lescalloy® 4330+V VAC-ARC High Strength Alloy Steel LESCALLOY 4330+V VAC-ARC steel is a modification of 4330 steel with hardenability and other properties improved by the addition of vanadium. It is a low alloy steel capable of being heat treated to .. |
|||
Tensile Strength, Ultimate | 1620 MPa | 235000 psi | |
Specialty Materials Hy-Bor 100 Boron/Graphite Hybrid Prepreg Tape Lower cost Hy-Bor version. Combining Specialty Materials' boron fiber with graphite prepreg, Hy-Bor® is a high-performance material with exceptional properties. Available with 4.0 and 5.6 m.. |
|||
Tensile Strength, Ultimate | 1620 MPa | 235000 psi | |
Elgiloy® Co-Cr-Ni Alloy, Strip, 50% Cold Reduction The strength, elongation, and hardness values are specific to this cold reduction treatment; other values below are typical of Elgiloy®.General Elgiloy® information: High strength, ductility, fati.. |
|||
Tensile Strength, Ultimate | 1620 MPa | 235000 psi | hardness of 48 HRC |
Bohler-Uddeholm UDDEHOLM QRO® 90 SUPREME Hot Work Tool Steel Chromium-molybdenum-vanadium alloyed steelQRO® 90 SUPREME is a premium hot work die steel with high hot yield strength and very good temper resistance. Especially suited for die casting of aluminum.. |
|||
Tensile Strength, Ultimate | 1620 MPa | 235000 psi | |
AK Steel 17-7 PH® Precipitation Hardening Stainless Steel, Condition RH 950 AK Steel 17-7 PH® provides high strength and hardness, excellent fatigue properties, good corrosion resistance, good formability, and minimum distortion upon heat treatment. This alloy provides va.. |
|||
Tensile Strength, Ultimate | 1620 MPa | 235000 psi | R<sub>m</sub>. 48 HRC. |
Assab Steels QRO 90 SUPREME Hot Work Steel QRO 90 SUPREME is a high-performance, chromium-molybdenum-vanadium alloyed hot-work tool steel which is characterized by: Excellent high temperature strength and hot hardnessVery good temper resista.. |
|||
Tensile Strength, Ultimate | 1620 MPa | 235000 psi | |
Carpenter Custom Age 625 PLUS® Nickel-Base Alloy, Cold Drawn 37.5% Data provided by Carpenter Technology Corporation.Custom Age 625 PLUS® alloy is a precipitation hardenable, nickel-base alloy which, in many environments, displays corrosion resistance similar to t.. |
|||
Tensile Strength, Ultimate | 1620 MPa | 235000 psi | 67.3% cold reduction |
ATI Allegheny Ludlum AL 2003™ Duplex Stainless Steel Characteristics: superior stress corrosion cracking resistance to Types 316 and 317, yield strength double that of conventional austenitic stainless steel, good corrosion resistance, good chloride s.. |