Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 1620 MPa
235000 psi
282°C Temper Temperature
Latrobe Lescalloy® 4330+V VAC-ARC High Strength Alloy Steel
LESCALLOY 4330+V VAC-ARC steel is a modification of 4330 steel with hardenability and other properties improved by the addition of vanadium. It is a low alloy steel capable of being heat treated to ..
Tensile Strength, Ultimate 1620 MPa
235000 psi
Specialty Materials Hy-Bor 100 Boron/Graphite Hybrid Prepreg Tape
Lower cost Hy-Bor version. Combining Specialty Materials' boron fiber with graphite prepreg, Hy-Bor® is a high-performance material with exceptional properties. Available with 4.0 and 5.6 m..
Tensile Strength, Ultimate 1620 MPa
235000 psi
Elgiloy® Co-Cr-Ni Alloy, Strip, 50% Cold Reduction
The strength, elongation, and hardness values are specific to this cold reduction treatment; other values below are typical of Elgiloy®.General Elgiloy® information: High strength, ductility, fati..
Tensile Strength, Ultimate 1620 MPa
235000 psi
hardness of 48 HRC
Bohler-Uddeholm UDDEHOLM QRO® 90 SUPREME Hot Work Tool Steel
Chromium-molybdenum-vanadium alloyed steelQRO® 90 SUPREME is a premium hot work die steel with high hot yield strength and very good temper resistance. Especially suited for die casting of aluminum..
Tensile Strength, Ultimate 1620 MPa
235000 psi
AK Steel 17-7 PH® Precipitation Hardening Stainless Steel, Condition RH 950
AK Steel 17-7 PH® provides high strength and hardness, excellent fatigue properties, good corrosion resistance, good formability, and minimum distortion upon heat treatment. This alloy provides va..
Tensile Strength, Ultimate 1620 MPa
235000 psi
R<sub>m</sub>. 48 HRC.
Assab Steels QRO 90 SUPREME Hot Work Steel
QRO 90 SUPREME is a high-performance, chromium-molybdenum-vanadium alloyed hot-work tool steel which is characterized by: Excellent high temperature strength and hot hardnessVery good temper resista..
Tensile Strength, Ultimate 1620 MPa
235000 psi
Carpenter Custom Age 625 PLUS® Nickel-Base Alloy, Cold Drawn 37.5%
Data provided by Carpenter Technology Corporation.Custom Age 625 PLUS® alloy is a precipitation hardenable, nickel-base alloy which, in many environments, displays corrosion resistance similar to t..
Tensile Strength, Ultimate 1620 MPa
235000 psi
67.3% cold reduction
ATI Allegheny Ludlum AL 2003™ Duplex Stainless Steel
Characteristics: superior stress corrosion cracking resistance to Types 316 and 317, yield strength double that of conventional austenitic stainless steel, good corrosion resistance, good chloride s..