Description: Static Control SheetInformation provided by Spartech.
Physical Properties Metric English Comments
Specific Gravity 1.07 g/cc
1.07 g/cc
ASTM D792
Mechanical Properties Metric English Comments
Hardness, Rockwell R 75
75
ASTM D785
Tensile Strength, Yield 20.7 MPa
3000 psi
ASTM D638
Flexural Modulus 1.38 GPa
200 ksi
ASTM D790
Izod Impact, Unnotched 2.67 J/cm
5.00 ft-lb/in
ASTM D256
Falling Dart Impact 271 J

@Temperature -40.0 °C
200 ft-lb

@Temperature -40.0 °F
ASTM D5420
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 83.9 °C
183 °F
ASTM D648
Electrical Properties Metric English Comments
Surface Resistivity per Square <= 1e+05
<= 1e+05
ASTM D257