Solvay TECHNYLSTARâ„¢ SX 216 L2 V60 PA6, 60% glass filled, DRY

Category Polymer , Thermoplastic , Nylon , Nylon 6 , Nylon 6, 60% Glass Fiber Filled
Manufacturer Solvay
Trade Name TECHNYLSTAR™
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Solvay TECHNYLSTARâ„¢ SX 216 L2 V60 PA6, 60% glass filled, DRY.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description: TECHNYLSTAR polyamide reinforced with 60% of glass fiber, UV stabilized and characterized by a high fluidity of the melt, for injection molding.Available in: Europe and North America Product Applications: TECHNYLSTAR TM SX 216 L2 V60 is suitable for all applications where a high rigidity is required. Due to its outstanding flow properties, the material easily fills the mould and the surface aspect of the finished part is excellent. Due to its high UV protection, this material can be used for paintless parts in automotive interior applications. This product is available in natural.Information provided by Rhodia, Rhodia has been acquired by Solvay.
Physical Properties Metric English Comments
Density 1.68 g/cc
0.0607 lb/in³
ISO 1183/A
Mechanical Properties Metric English Comments
Tensile Strength at Break 220 MPa
31900 psi
ISO 527 Type 1A
Elongation at Break 2.5 %
2.5 %
ISO 527 Type 1A
Tensile Modulus 18.7 GPa
2710 ksi
ISO 527 Type 1A
Izod Impact, Notched (ISO) 19.6 kJ/m²
9.33 ft-lb/in²
ISO 180/1eA
Izod Impact, Unnotched (ISO) 81.1 kJ/m²
38.6 ft-lb/in²
ISO 180/1eU
Charpy Impact Unnotched 8.26 J/cm²
39.3 ft-lb/in²
ISO 179/1eU
Charpy Impact, Notched 1.49 J/cm²
7.09 ft-lb/in²
ISO 179/1eA
Processing Properties Metric English Comments
Moisture Content <= 0.15 %
<= 0.15 %