Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Saint-Gobain Tygon® Transflow S3™ M-34-R Raw Milk Dairy Tubing Formulation

Category Polymer , Thermoplastic
Manufacturer Saint-Gobain Perfomance Plastics
Trade Name Tygon®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Saint-Gobain Tygon® Transflow S3™ M-34-R Raw Milk Dairy Tubing Formulation.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Transflow S3™ M-34-R tubing, from Saint-Gobain Performance Plastics, is now phthalate-free. Saint-Gobain is proud to be among the first companies to offer sustainable flexible tubing products. The bio-based Transflow S3™ line combines the high performance standards customers demand with an eco-friendly tubing design. Transflow S3™ Raw Milk tubing is specially formulated to reduce the risks that can occur with the use of rubber tubings. Many regulatory sanitarians throughout the world recognize Transflow S3™ as the preferred tubing for raw milk transfer. Long lasting Transflow S3™ tubing is extremely flexible and installs quickly and easily around stantions and milk handling equipment. It resists embrittlement and cracking from oxidation that often shortens the service life of other tubings. The same reliability and performance found in Transflow S3™ Raw Milk tubing is also available for tank truck operators. Produced in large bore sizes up to 3" I.D., Transflow tubings' clarity, flexibility and cleanability are ideally suited for bulk milk transfer. Transflow S3™ is also produced in single and twin tube confiations ideally suited for supply air transport. It's smooth inner surface is less susceptible to particle entrapment which can restrict air flow while crystal clarity permits detection of equipment deficiencies such as backflow of milk into the air lines. Every foot of Transflow S3™ Raw Milk tubing has been embedded with a trademark blue stripe within the tubing walls. The embedded blue stripe is your assurance of receiving genuine Transflow tubing, the worlds' finest raw milk tubing produced specifically for the dairy industry. Features and Benefits Crystal clarity permits visual inspection of milk flow Smooth, non-porous bore resists buildup Lightweight and flexible for quick installationNon-wetting properties allow easy cleaning and complete drainage Durability for long and reliable service Contains no BPA or phthalates Regulatory Standards Transflow S3™ complies with FDA, NSF, #-A, Japan Food Sanitation Law # 370/1959, REACH, 1935/2004/EC and 10/2011/EU for many foods and beverages. Transflow S3™ tubing products do not contain chemicals listed in California's Prop 65.Information provided by Saint Gobain Performance Products.
Physical Properties Metric English Comments
Specific Gravity 1.21 g/cc
1.21 g/cc
ASTM D792
Water Absorption 0.22 %

@Temperature 22.8 °C,
Time 86400 sec
0.22 %

@Temperature 73.0 °F,
Time 24.0 hour
ASTM D570
Mechanical Properties Metric English Comments
Hardness, Shore A 66

@Time 15.0 sec
66

@Time 0.00417 hour
ASTM D2240
Tensile Strength 15.2 MPa
2200 psi
ASTM D412
Tensile Strength, Yield 9.501 MPa

@Strain 200 %
1378 psi

@Strain 200 %
Elongation at Break 390 %
390 %
ASTM D412
Tear Strength 43.8 kN/m
250 pli
ASTM D1004
Compression Set 59 %

@Temperature 70.0 °C,
Time 79200 sec
59 %

@Temperature 158 °F,
Time 22.0 hour
ASTM D395 Method B
Tensile Set 57 %
57 %
ASTM D412
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 73.9 °C
165 °F
Brittleness Temperature -36.1 °C
-33.0 °F
ASTM D746
Optical Properties Metric English Comments
Transmission, Visible 90 %
90 %
Clear, but value not quantified
Compliance Properties Metric English Comments
FDA Yes
Yes
NSF Yes
Yes
Descriptive Properties Value Comments
Color Clear
Users viewing this material also viewed the following: