Polymer Property : Izod Impact, Unnotched (ISO) = 81.1 kJ/m² Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Izod Impact, Unnotched (ISO) 81.1 kJ/m²
38.6 ft-lb/in²
ISO 180/1eU
Solvay TECHNYLSTARâ„¢ SX 216 L2 V60 PA6, 60% glass filled, DRY
Description: TECHNYLSTAR polyamide reinforced with 60% of glass fiber, UV stabilized and characterized by a high fluidity of the melt, for injection molding.Available in: Europe and North America Pr..