Polymer Property : Tensile Modulus = 2710 ksi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Modulus 18.7 GPa
2710 ksi
ISO 527 Type 1A
Solvay TECHNYLSTARâ„¢ SX 216 L2 V60 PA6, 60% glass filled, DRY
Description: TECHNYLSTAR polyamide reinforced with 60% of glass fiber, UV stabilized and characterized by a high fluidity of the melt, for injection molding.Available in: Europe and North America Pr..
Tensile Modulus 18.7 GPa
2710 ksi
1 mm/min; ISO 527
SABIC Innovative Plastics LNP STAT-KON RX05488 PA 66
LNP STAT-KON* RX05488 is a compound based on Nylon 66 resin containing Carbon Fiber, Flame Retardant, Glass Fiber, PTFE. Added features of this material include: Electrically Conductive.
Tensile Modulus 18.7 GPa
2710 ksi
1 mm/min; ISO 527
SABIC Innovative Plastics LNP THERMOCOMP QC006 PA6.10 (Europe-Africa-Middle East)
LNP * THERMOCOMP* QC006 is a compound based on PA610 resin containing Carbon Fiber. Added features include; Electrically Conductive.
Tensile Modulus 18.7 GPa
2710 ksi
1mm/min; ISO 527
BASF Ultradur B 4040 G10 LS High Speed BK15029 50% Glass Filled PBT/PET
Tensile Modulus 18.7 GPa
2710 ksi
ISO 527-1/-2
BASF Ultradur® B 4040 G10 50% Glass Filled BK 15029 PBT + PET
Description: Injection molding grade with 50% glass fibers for industrial parts with excellent surface quality, for example external door handles in vehicles, visible sunroof frames, oven door handl..