Solvay TECHNYLSTARâ„¢ A205 F Natural S PA6, Eh 0

Category Polymer , Thermoplastic , Nylon , Nylon 66 , Nylon 66, Unreinforced
Manufacturer Solvay
Trade Name TECHNYLSTAR™
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Solvay TECHNYLSTARâ„¢ A205 F Natural S PA6, Eh 0.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description: TECHNYLSTAR A205 F NATURAL S is a polyamide 6.6 with low viscosity for fast cycle molding.Colors: it is supplied in natural color.Available in: Latin America and North AmericaMain Properties: High Fluidity, V2 UL 94 Classification and Glow wire Resistance Applications: This product is indicated for various applications at automotive and electric & electronic industries. Information provided by Rhodia, Rhodia has been acquired by Solvay.
Physical Properties Metric English Comments
Density 1.15 g/cc
0.0415 lb/in³
ISO 1183/A
Mechanical Properties Metric English Comments
Tensile Strength at Break 80.0 MPa
11600 psi
ISO 527
Elongation at Break 32 %
32 %
ISO 527
Tensile Modulus 3.30 GPa
479 ksi
ISO 527
Flexural Modulus 3.07 GPa
445 ksi
ISO 178
Izod Impact, Notched (ISO) 3.50 kJ/m²
1.67 ft-lb/in²
ISO 180
Charpy Impact Unnotched NB
NB
ISO 179
Charpy Impact, Notched 0.340 J/cm²
1.62 ft-lb/in²
ISO 179
Thermal Properties Metric English Comments
Melting Point 262 °C
504 °F
ASTM D3418
Deflection Temperature at 1.8 MPa (264 psi) 69.0 °C
156 °F
ISO 75
Flammability, UL94 V-2

@Thickness 1.60 mm
V-2

@Thickness 0.0630 in
Glow Wire Test 960 °C
1760 °F
CEI 695
Electrical Properties Metric English Comments
Volume Resistivity 1.00e+14 ohm-cm
1.00e+14 ohm-cm
CEI 93
Dielectric Constant 2.9
2.9
CEI 250
Dielectric Strength 27.0 kV/mm
686 kV/in
CEI 93
Dissipation Factor 0.030
0.030
CEI 250
Comparative Tracking Index 600 V
600 V
CEI 112
Processing Properties Metric English Comments
Feed Temperature 265 - 275 °C
509 - 527 °F
Mold Temperature 60.0 - 80.0 °C
140 - 176 °F
Descriptive Properties Value Comments
Compression Zone 270-285°C
Mixing Zone 270-285°C