Mechanical Properties Metric English Comments
Flexural Modulus 3.07 GPa
445 ksi
2 mm/min; ISO 178
SABIC Innovative Plastics EXTEM VH1003M PEI Copolymer
Transparent, Thermoplastic Polyimide (TPI) resin with a glass transition temperature (Tg) of 247C. Internal mold release. This product has thinwall FR capability and has a UL94 V0 listing. This mate..
Flexural Modulus 3.07 GPa
445 ksi
2 mm/min; ISO 178
SABIC Innovative Plastics EXTEM VH1003M PEI Copolymer (Asia Pacific)
Transparent, Thermoplastic Polyimide (TPI) resin with a glass transition temperature (Tg) of 247C. Internal mold release. This product has thinwall FR capability and has a UL94 V0 listing. This mate..
Flexural Modulus 3.07 GPa
445 ksi
2 mm/min; ISO 178
SABIC Innovative Plastics EXTEM VH1003M PEI Copolymer (Europe-Africa-Middle East)
Transparent, Thermoplastic Polyimide (TPI) resin. Glass transition Temp. (Tg) of 247°C. Internal mold release. This resin has thinwall FR capability and has a UL94 V0 listing. Resin is halogen free..
Flexural Modulus 3.07 GPa
445 ksi
ASTM D790
Quadrant EPP Acetron® AF Blend POM-H Acetal Extruded PTFE-Filled Acetal Homopolymer (ASTM Product Data Sheet)
Flexural Modulus 3.07 GPa
445 ksi
ASTM D790
Polymer Resources ABS-G10 ABS, 10% Glass Reinforced
Acrylonitrile Butadiene Styrene, 10% Glass ReinforcedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information..
Flexural Modulus 3.07 GPa
445 ksi
at 0.05 in/min; ASTM D790
M. Holland Company GS410WC Polystyrene  (discontinued **)
Features: High Clarity, High FlowUses: Household Goods, LabwareApprovals: FDA 21 CFR 177.1640 Processing Method: Injection MoldingInformation provided by M. Holland.
Flexural Modulus 3.07 GPa
445 ksi
Ineos Styrenics Polystyrene 147F (NAFTA)
An easy flow, general purpose polystyrene. Has moderate heat resistance and strength for general molding and extrusion applications.Information provided by BASF.Ineos Styrenics purchased this produ..
Flexural Modulus 3.07 GPa
445 ksi
2 mm/min; ISO 178
SABIC Innovative Plastics LNP LUBRICOMP KAL22 Acetal Copolymer
LNP* LUBRICOMP* KAL22 is a compound based on Acetal Copolymer resin containing 10% PTFE, 10% Aramid Fiber. Added feature of this material is: Wear Resistant.
Flexural Modulus 3.07 GPa
445 ksi
1.3 mm/min, 50 mm span; ASTM D790
SABIC Innovative Plastics LNP LUBRICOMP LL002 PEEK
LNP* LUBRICOMP* LL002 is a compound based on Polyetheretherketone containing 10% PTFE. Added feature of this material is: Wear Resistant.
Flexural Modulus 3.07 GPa
445 ksi
ISO 178
Solvay TECHNYLSTARâ„¢ A205 F Natural S PA6, Eh 0
Description: TECHNYLSTAR A205 F NATURAL S is a polyamide 6.6 with low viscosity for fast cycle molding.Colors: it is supplied in natural color.Available in: Latin America and North AmericaMain Prope..
Flexural Modulus 3.07 GPa
445 ksi
2 mm/min; ISO 178
SABIC Innovative Plastics Ultem AUT230M PEI
Transparent polyetherimide (Tg 247 degC). Contains low level of mold release. Very low outgassing and plateout, for automotive lighting applications where highly metallized, reflective surfaces are ..
Flexural Modulus 3.07 GPa
445 ksi
2 mm/min; ISO 178
SABIC Innovative Plastics Ultem AUT230M PEI (Asia Pacific)
Transparent polyetherimide (Tg 247 degC) with internal mold release. Very low outgassing and plateout for automotive lighting applications where highly metallized, reflective surfaces are required...
Flexural Modulus 3.07 GPa
445 ksi
2 mm/min; ISO 178
SABIC Innovative Plastics Ultem AUT230M PEI (Europe-Africa-Middle East)
Transparent polyetherimide (Tg 247 degC) with internal mold release. Very low outgassing and plateout for automotive lighting applications where highly metallized, reflective surfaces are required...
Flexural Modulus 3.07 GPa
445 ksi
2 mm/min; ISO 178
SABIC Innovative Plastics ULTEM XH6050M PEI Copolymer
Enhanced flow Polyetherimidesulfone copolymer (Tg 247C) with internal mold release. ECO Conforming, UL94 V0 listing. Resin is subject to U.S. Commerce Control Laws (15CFR Chapter VII, Part 774).
Flexural Modulus 3.07 GPa
445 ksi
2 mm/min; ISO 178
SABIC Innovative Plastics Ultem XH6050M PEI Copolymer (Europe-Africa-Middle East)
Enhanced flow Polyetherimidesulfone copolymer (Tg 247C) with internal mold release. ECO Conforming, UL94 V0 listing. Resin is subject to U.S. Commerce Control Laws (15CFR Chapter VII, Part 774).Thi..
Flexural Modulus 3.07 GPa
445 ksi
2 mm/min; ISO 178
SABIC Innovative Plastics ULTEM XH6050M PEI Copolymer (Asia Pacific)
Enhanced flow Polyetherimidesulfone copolymer (Tg 247C) with internal mold release. ECO Conforming, UL94 V0 listing. Resin is subject to U.S. Commerce Control Laws (15CFR Chapter VII, Part 774).
Flexural Modulus 3.07 GPa
445 ksi
ASTM D-790
Axiall 7751 Rigid PVC, Extrusion
Georgia Gulf 7751 is a vertical blind profile exterior compound requiring the following properties: Impact Strength & ToughnessColorabilityDimensional StabilityUV Color StabilityEasy Processing in ..
Flexural Modulus 3.07 GPa
445 ksi
ASTM D790
Aaron Industries AAROPRENE® GFPP 2020 Glass Filled Polypropylene
AAROPRENE® GFPP 2000 Series Glass Reinforced CompoundsMelt flow index may be specified. Color may be specified.
Copyright © lookpolymers.com All Rights Reserved