Solvay TECHNYL® eXten D247 F Nylon 66 & 610

Category Polymer , Thermoplastic , Nylon
Manufacturer Solvay
Trade Name Technyl®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Solvay TECHNYL® eXten D247 F Nylon 66 & 610.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description: Polyamid 66 & 610, impact modified, alkali resistance, mold release, for injection molding. This material is available in natural color and in colors on requestAvailable in: Asia Pacific, Europe, Latin America and North AmericaProduct Applications: TECHNYL® eXten D 247 is used in all sectors of industry, offering high impact strength & excellent productivity. This product is especially suitable for the following purposes: Battery gaskets.Information provided by Rhodia, Rhodia has been acquired by Solvay.
Physical Properties Metric English Comments
Density 1.08 g/cc
0.0390 lb/in³
ISO 1183
Mechanical Properties Metric English Comments
Hardness, Rockwell R 111
111
ASTM D786
Tensile Strength, Yield 60.0 MPa
8700 psi
ASTM D638
Elongation at Break 40 %
40 %
ASTM D638
Flexural Strength 90.0 MPa
13100 psi
ASTM D790
Flexural Modulus 2.60 GPa
377 ksi
ASTM D790
Izod Impact, Notched 2.10 J/cm
3.93 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Melting Point 262 °C
504 °F
ISO 11357
Deflection Temperature at 0.46 MPa (66 psi) 182 °C
360 °F
ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 68.0 °C
154 °F
ASTM D648
Flammability, UL94 HB

@Thickness 3.20 mm
HB

@Thickness 0.126 in
ISO 1210
Processing Properties Metric English Comments
Feed Temperature 265 - 270 °C
509 - 518 °F
Mold Temperature 60.0 - 80.0 °C
140 - 176 °F
Drying Temperature 80.0 °C
176 °F
Moisture Content <= 0.20 %
<= 0.20 %
Descriptive Properties Value Comments
Compression Zone 270-280°C
Mixing Zone 280-290°C