Thermal Properties | Metric | English | Comments |
---|---|---|---|
Deflection Temperature at 0.46 MPa (66 psi) | 182 °C | 360 °F | ASTM D648 |
Nylene® 401D, Nylon 6 Injection molding grade. Dry as molded. Nylene 401D is a specially formulated nylon 6 molding resin possessing outstanding flow characteristics. Nylene 401D is ideally suited for applications requi.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 182 °C | 360 °F | ASTM D648 |
Nylene® 404 Nylon 6 Injection molding grade. Dry as molded. Nylene 404 is a heat stabilized version of 401 which is recommended for general purpose nylon molding applications in both thin and heavy sections. In additi.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 182 °C | 360 °F | ISO 75, ASTM D648 |
Nilit Nilitop BT N Unfilled, Nucleated PBT Description: Nilitop BT N is an unfilled, nucleated PBT that has excellent cycle times.Key characteristics: Good overall mechanical performanceLow moisture absorptionExcellent UV resistanceExcellent.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 182 °C | 360 °F | ISO 75-1/-2 |
Lanxess Durethan® DP BM 410 H2.0 901510 Nylon 6, 10% Mineral + Glass Fiber PA 6, injection molding grade, 10% glass fibers/mineral, good heat-ageing resistance |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 182 °C @Thickness 3.20 mm |
360 °F @Thickness 0.126 in |
unannealed; ASTM D648 |
SABIC Innovative Plastics LNP LUBRICOMP HFG25Z PA 11 (Asia Pacific) LNP* Lubricomp* HFG25Z is a compound based on Nylon 11 resin containing Glass Fiber, Graphite Powder. Added features of this material include: Internally Lubricated. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 182 °C | 360 °F | ASTM D648 |
Solvay TECHNYL® eXten D247 F Nylon 66 & 610 Description: Polyamid 66 & 610, impact modified, alkali resistance, mold release, for injection molding. This material is available in natural color and in colors on requestAvailable in: Asia Pacifi.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 182 °C | 360 °F | ASTM D648 |
UBE UBESTA® 3020GX6 Glass Fiber Reinforced Nylon 12 Description: UBE UBESTA® Automotive grade Nylon 12Comments: conductive, glass fiber reinforced, UV resistanceInformation provided by UBE. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 182 °C | 360 °F | ASTM D648 |
Chase Plastics CP Pryme® N100HSL (COND, 50% RH) Nylon 6, Heat Stabilized, Internally Lubricated Information provided by Chase Plastics. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 182 °C | 360 °F | ASTM D648 |
Chase Plastics CP Pryme® N100L (DAM) Nylon 6, Internally Lubricated Information provided by Chase Plastics. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 182 °C | 360 °F | ASTM D648 |
A. Schulman SCHULADUR® A GB30 30% Glass Bead Reinforced PBT Information provided by A. Schulman. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 182 °C | 360 °F | ASTM D648 |
A. Schulman SCHULADUR® A GB30 30% Glass Bead Reinforced PBT Information provided by A. Schulman. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 182 °C | 360 °F | ASTM D648 |
A. Schulman SCHULADUR® A GB30 30% Glass Bead Reinforced PBT Information provided by A. Schulman. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 182 °C | 360 °F | ISO-R 75 Method B |
Hippe PEEK Polyetheretherketone PEEK is a crystalline, easily machinable thermoplastic which is characterized by high tensile and constant good electrical properties between 0°-220°C, as well as due to favorable tribological beh.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 182 °C | 360 °F | ASTM D648 |
E-Polymers TEKAMID® JN110 PPE+PA66 Filler Reinforced PA/PPE Alloy Polyamide (Nylon) Resin. TEKAMID is widely being used in manufacturing of automotive and industrial parts with its outstanding mechanical, thermal and chemical properties.JN-series: PA66/PPE, PA6/P.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 182 °C | 359 °F | ASTM D648 |
Aclo Accucomp Nylon 66 NY0750L |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 182 °C | 360 °F | ASTM D648 |
Adell BH-18 Nylon 6, 40% Mineral Filled Data provided by Adell Plastics, Inc. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 182 °C | 360 °F | ASTM D648 |
Ashley Polymers Ashlene® 829 Nylon 6 Basic Nylon 6, low viscosity, unlubricated.Data provided by the manufacturer |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 182 °C | 360 °F | ASTM D648 |
Ashley Polymers Ashlene® 829L Nylon 6 Basic Nylon 6, low viscosity, lubricated.Data provided by the manufacturer |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 182 °C | 360 °F | ASTM D648 |
Ashley Polymers Ashlene® 829LF Nylon 6 Basic Nylon 6, low viscosity, lubricated. This is FDA approved.Data provided by the manufacturer |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 182 °C | 360 °F | ASTM D648 |
Ashley Polymers Ashlene® 835 Nylon 6 Basic Nylon 6 high viscosity, for coating and laminating applications, FDA approved.Data provided by the manufacturer |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 182 °C | 360 °F | ASTM D648 |
Aaron Industries AAROPRENE® AEN 6000-1 Nylon 6 Engineered Resin |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 182 °C | 360 °F | ASTM D648 |
Chase Plastics CP Pryme® N200L (DAM) Nylon 6, Internally Lubricated Information provided by Chase Plastics. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 182 °C | 360 °F | ASTM D648 |
Quantum PEEK Information provided by Quantum Advanced Engineering Plastics |