Solvay TECHNYL® C 502XT PA6, Conditioned

Category Polymer , Thermoplastic , Nylon , Nylon 6 , Nylon 6, Extruded
Manufacturer Solvay
Trade Name Technyl®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Solvay TECHNYL® C 502XT PA6, Conditioned.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description: Unreinforced polyamide 6, very high viscosity, for extrusion.Available in: Europe Product Applications: It is suitable for extruded semi-finished products, such as: Rods, profiles, sheets, pipes. All the semi-finished products can be machined without special treatment, such as: Precision gears, bolts, etc. This product is available in natural.Information provided by Rhodia, Rhodia has been acquired by Solvay.
Physical Properties Metric English Comments
Density 1.13 g/cc
0.0408 lb/in³
ISO 1183/A
Mechanical Properties Metric English Comments
Tensile Strength, Yield 35.0 MPa
5080 psi
ISO 527 type 1 A
Elongation at Break 300 %
300 %
ISO 527 Type 1A
Elongation at Yield 2.5 %
2.5 %
ISO 527 type 1 A
Tensile Modulus 0.900 GPa
131 ksi
ISO 527 Type 1A
Izod Impact, Notched (ISO) NB
NB
ISO 180/1eA
Charpy Impact Unnotched NB
NB
ISO 179/1eU
Electrical Properties Metric English Comments
Volume Resistivity 1.00e+10 ohm-cm
1.00e+10 ohm-cm
IEC 60093
Surface Resistance 1.00e+10 ohm
1.00e+10 ohm
IEC 60093
Dielectric Constant 3.9
3.9
IEC 60250
Dielectric Strength 18.0 kV/mm
457 kV/in
IEC 60243
Dissipation Factor 0.10
0.10
IEC 60250