Material Notes:
Cogegum® HFFR -Halogen Free Fire Retardant compound. Polyolefin based thermoplastic compound containing a fire retardant system that contributes to give the cable self-extinguish properties without halogenidric acids evolution; furthermore, toxic and corrosive gases emission and smoke generation are particularly reduced. These characteristics make this compound suitable in all applications where the fire behavior of cable materials is one of the main concerns to be considered in establishing a high safety level in public places.Features: Flame Retardant; Halogen Free; Low Smoke Emission; Low Toxicity; Self ExtinguishingUses: Cable Jacketing; Low Voltage Insulation; Wire & Cable ApplicationsExtrusion equipment: standard extruders for thermoplastics equipped with low compression screw (1:1.2-1.4 compression ratio and 20-25 L/D ratio are suggested), and an adequate barrel thermoregulation.Additional Properties: Bending Test - IEC 60811 (-25°C): Pass; Calorific Potential - ISO 1716 17.5 MJ/kg; Cold Impact - IEC 60811 (-25°C): Pass; Collar Temperature - 170 to 180 °C; Corrosive Gas in Smoke - IEC 60754-2 < 10.0 µS/mm; Corrosive Gas in Smoke - IEC 60754-2 > 4.30; Halogenidric Acid Emissions - IEC 60754-1 < 0.10 %; Head Temperature - 180 to 190 °C; Heat Shock - IEC 60811 (150°C): Pass; Hot Pressure Test - IEC 60811 (90°C): < 50 %; Insulation Resistance Constant - IEC 60502 (20°C): 4000 Mohm·km; Insulation Resistance Constant - IEC 60502 (90°C): 1000 Mohm·km; Temperature Index (Burning) - NES 715 280 °C; Water Absorption - IEC 60811 (100°C): 1.20 mg/cm²Information provided by Solvay Specialty Polymers.
Physical Properties Metric English Comments
Density 1.44 g/cc
0.0520 lb/in³
ASTM D792
Environmental Stress Crack Resistance >= 1000 hour

@Thickness 3.00 mm,
Temperature 50.0 °C
>= 1000 hour

@Thickness 0.118 in,
Temperature 122 °F
Condition A, Compression Molded, 10% Igepal; ASTM D1693
Melt Flow 4.5 g/10 min

@Load 21.6 kg,
Temperature 190 °C
4.5 g/10 min

@Load 47.6 lb,
Temperature 374 °F
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Shore D 50
50
ISO 868
Tensile Strength at Break 12.5 MPa
1810 psi
ASTM D638
Elongation at Break 200 %
200 %
ASTM D638
Thermal Properties Metric English Comments
Oxygen Index 30 %
30 %
ASTM D2863
Electrical Properties Metric English Comments
Volume Resistivity 2.70e+14 ohm-cm

@Temperature 90.0 °C
2.70e+14 ohm-cm

@Temperature 194 °F
ASTM D257
1.00e+15 ohm-cm

@Temperature 20.0 °C
1.00e+15 ohm-cm

@Temperature 68.0 °F
ASTM D257
Processing Properties Metric English Comments
Zone 1 140 - 160 °C
284 - 320 °F
Zone 2 150 - 170 °C
302 - 338 °F
Zone 3 160 - 180 °C
320 - 356 °F
Zone 4 170 - 180 °C
338 - 356 °F
Die Cooling Temperature 180 - 200 °C
356 - 392 °F
Descriptive Properties Value Comments
Availability Asia Pacific
Europe
North America
RoHS Compliance RoHS Compliant
Users viewing this material also viewed the following: