Electrical Properties | Metric | English | Comments |
---|---|---|---|
Volume Resistivity | 2.70e+14 ohm-cm @Temperature 90.0 °C |
2.70e+14 ohm-cm @Temperature 194 °F |
IEC 60502 |
Solvay Specialty Polymers Cogegum® AFR/960 Polyolefin, Unspecified
(Unverified Data**) Cogegum® HFFR -Halogen Free Fire Retardant compound Polyolefin based thermoplastic compound containing a fire retardant system that contributes to give the cable self-extinguish properties without .. |
|||
Volume Resistivity | 2.70e+14 ohm-cm @Temperature 90.0 °C |
2.70e+14 ohm-cm @Temperature 194 °F |
ASTM D257 |
Solvay Specialty Polymers Polidiemme® G/400 Thermoset Elastomer (TSE) Elastomer based compound crosslinkable by ambient moisture, consisting of a silane pregrafted base compound to be used with a catalyst masterbatch (Sioplas® method).Standards complying: Cenelec H.. |
|||
Volume Resistivity | 2.70e+14 ohm-cm @Temperature 90.0 °C |
2.70e+14 ohm-cm @Temperature 194 °F |
ASTM D257 |
Solvay Specialty Polymers Cogegum® AFR/960 Polyolefin Cogegum® HFFR -Halogen Free Fire Retardant compound. Polyolefin based thermoplastic compound containing a fire retardant system that contributes to give the cable self-extinguish properties withou.. |