Processing Properties | Metric | English | Comments |
---|---|---|---|
Zone 4 | 170 - 180 °C | 338 - 356 °F | |
Solvay Specialty Polymers Cogegum® AFR/920 Polyolefin, Unspecified
(discontinued **) Cogegum® HFFR -Halogen Free Fire Retardant compound Polyolefin based thermoplastic compound containing a fire retardant system that contributes to give the cable self-extinguish properties without .. |
|||
Zone 4 | 170 - 180 °C | 338 - 356 °F | |
Solvay Specialty Polymers Cogegum® AFR/920-UV Polyolefin, Unspecified
(Unverified Data**) Cogegum® HFFR -Halogen Free Fire Retardant compound Polyolefin based thermoplastic compound containing a fire retardant system that contributes to give the cable self-extinguish properties without .. |
|||
Zone 4 | 170 - 180 °C | 338 - 356 °F | |
Solvay Specialty Polymers Cogegum® AFR/930 Polyolefin, Unspecified
(discontinued **) Cogegum® HFFR -Halogen Free Fire Retardant compound Polyolefin based thermoplastic compound containing a fire retardant system that contributes to give the cable self-extinguish properties without .. |
|||
Zone 4 | 170 - 180 °C | 338 - 356 °F | |
Solvay Specialty Polymers Cogegum® AFR/960 Polyolefin, Unspecified
(Unverified Data**) Cogegum® HFFR -Halogen Free Fire Retardant compound Polyolefin based thermoplastic compound containing a fire retardant system that contributes to give the cable self-extinguish properties without .. |
|||
Zone 4 | 170 - 180 °C | 338 - 356 °F | |
Lubrizol Advanced Materials Pearlbond® 12F75UV Thermoplastic Polyurethane Pearlbond™ 12F75UV is a UV-resistant standard polyester-based TPU supplied in form of translucent, colorless pellets, featuring a low melting point and very low gel content. Processed by extrus.. |
|||
Zone 4 | 170 - 180 °C | 338 - 356 °F | |
Lubrizol Advanced Materials Pearlbond® D1160 Thermoplastic Polyurethane Pearlbond™ D1160 is a linear, aromatic polyurethane, supplied in form of small white granules, which combines a high crystallization rate and high thermoplasticity level. Applications: Pearlbo.. |
|||
Zone 4 | 170 - 180 °C | 338 - 356 °F | |
Lubrizol Advanced Materials PEARLTHANE® 12F75UV Thermoplastic Polyurethane Elastomer PEARLTHANE® D12F75UV is a UV resistant standard polyester based TPU supplied in form of translucent, colorless or slightly yellowish pellets, featuring a low melting point and very low gel conten.. |
|||
Zone 4 | 170 - 180 °C | 338 - 356 °F | |
Solvay Specialty Polymers Cogegum® AFR/920-UV Polyolefin Flame Retardant; Good UV Resistance; Halogen Free; Low Smoke Emission; Low Toxicity; Self ExtinguishingUses: Cable Jacketing; Low Voltage Insulation; Wire & Cable ApplicationsExtrusion equipment: st.. |
|||
Zone 4 | 160 - 180 °C | 320 - 356 °F | |
Solvay Specialty Polymers Polidan® EC/110 Polyethylene, Crosslinked (XLPE) Polidan® XLPE-PEX -Cross-linkable Polyethylene. Low density polyethylene based compound crosslinkable by moisture; it consists of a silane pregrafted base compound (Sioplas® method) to be use.. |
|||
Zone 4 | 160 - 180 °C | 320 - 356 °F | |
Solvay Specialty Polymers Polidan® EC/51 Polyethylene, Crosslinked (XLPE) Flexible low density polyethylene based compound crosslinkable by moisture; it consists of a silane pregrafted base compound (Sioplas® method) to be used with a catalyst masterbatch.Standards com.. |
|||
Zone 4 | 170 - 180 °C | 338 - 356 °F | |
Solvay Specialty Polymers Cogegum® AFR/960 Polyolefin Cogegum® HFFR -Halogen Free Fire Retardant compound. Polyolefin based thermoplastic compound containing a fire retardant system that contributes to give the cable self-extinguish properties withou.. |