Mechanical Properties Metric English Comments
Shear Modulus 5.18 GPa
751 ksi
Calculated
Solvay Specialty Polymers Amodel® FR-4133 Polyphthalamide (PPA) Resin, 33% Glass Reinforced, at 50% RH  (disco
AMODEL FR-4133 is a 33% glass-reinforced polyphthalamide (PPA) resin designed for electrical and electronic applications. This UL94-V0 resin offers the highest mechanical and electrical properties, ..