Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Solvay Specialty Polymers Amodel® AT-6130 HS Polyphthalamide (PPA), 30% Glass Fiber (Conditioned)

Category Polymer , Thermoplastic , Polyphthalamide (PPA) , Polyphthalamide (PPA), 30% Glass Fiber Reinforced
Manufacturer Solvay Specialty Polymers
Trade Name Amodel®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Solvay Specialty Polymers Amodel® AT-6130 HS Polyphthalamide (PPA), 30% Glass Fiber (Conditioned).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Amodel® AT-6130 HS is a 30% glass-reinforced, toughened polyphthalamide (PPA) resin that has more elongation than other 30% glass-reinforced grades of Amodel® resin. This grade was developed for automotive snap-fit electronic connectors. It offers high flow and short molding cycles. The processing window is relatively broad and mold temperatures as low as 150°F (65°C) can be used.Features: Good Chemical Resistance; Good Flow; Good Wear Resistance; Heat Stabilized; High Heat Resistance; High Strength; Hot Water Moldability; Impact Modified; Low Friction; LubricatedUses: Automotive Applications; Automotive Electronics; Automotive Under the Hood; Bearings; Connectors; Fuel Lines; General Purpose; Housings; Industrial Applications; Industrial Parts; Lawn and Garden Equipment; Machine/Mechanical Parts; Metal Replacement; Valves/Valve PartsInjection Molding Notes: Amodel® compounds are shipped in moisture-resistant packages at moisture levels according to specifications. Sealed, undamaged bags should be preferably stored in a dry room at a maximum temperature of 50°C (122°F) and should be protected from possible damage. If only a portion of a package is used, the remaining material should be transferred into a sealable container. It is recommended that Amodel® resins be dried prior to molding.Automotive Specifications ASTM D4000 PPA0123 G30 KD150 KN080 PM095 PN095 YI255 LD002 Color: BK-324 Black; ASTM D4000 PPA0123 G30 KD150 KN080 PM095 PN095 YI255 LD002 Color: NT Natural; ASTM D6779 PA103G30; DELPHI MS 5218 Color: BK-324 Black; DELPHI MS 5218 Color: NT Natural; GM GMP.PPA.017 Color: BK-324 Black; GM GMP.PPA.017 Color: NT Natural; GM GMW16363P-PPA-GF30 Color: Black; GM GMW16363P-PPA-GF30 Color: Natural; ISO 1874-PA 6T/66-HI, MH, 11-090, GF30Information provided by Solvay Specialty Polymers.
Physical Properties Metric English Comments
Density 1.34 g/cc
0.0484 lb/in³
Dry; ISO 1183
Filler Content 30 %
30 %
Glass Fiber
Linear Mold Shrinkage, Flow 0.0050 cm/cm
0.0050 in/in
Dry
Linear Mold Shrinkage, Transverse 0.0080 cm/cm
0.0080 in/in
Dry; ASTM D955
Processing Properties Metric English Comments
Rear Barrel Temperature 316 - 324 °C
601 - 615 °F
Front Barrel Temperature 327 - 332 °C
621 - 630 °F
Melt Temperature 321 - 335 °C
610 - 635 °F
Mold Temperature 65.6 - 93.3 °C
150 - 200 °F
Drying Temperature 121 °C

@Time 14400 sec
250 °F

@Time 4.00 hour
Moisture Content <= 0.15 %
<= 0.15 %
Descriptive Properties Value Comments
Additive Heat Stabilizer
Impact Modifier
Lubricant
Mold Release
Availability Africa & Middle East
Asia Pacific
Europe
Latin America
North America
Color Black; Natural
Form Pellets
Injection Rate Fast
Processing Technique Water-Heated Mold Injection Molding
RoHS Compliance RoHS Compliant