Processing Properties Metric English Comments
Melt Temperature 321 - 335 °C
610 - 635 °F
Solvay Specialty Polymers Amodel® AT-6115 HS Polyphthalamide (PPA)  (Unverified Data**)
Amodel AT-6115 HS is a 15% glass-fiber reinforced, toughened grade of polyphthalamide (PPA) resin designed to possess more elongation than other 15% glass-fiber reinforced grades of Amodel resin. Th..
Melt Temperature 243 - 335 °C
469 - 635 °F
Average value: 305 °C Grade Count:7
Overview of materials for Polystyrene + Polyphenylene Ether, Glass + Mineral Filler
This property data is a summary of similar materials in the MatWeb database for the category "Polystyrene + Polyphenylene Ether, Glass + Mineral Filler". Each property range of values reported is mi..
Melt Temperature 305 - 335 °C
581 - 635 °F
Covestro Makrolon® CD 2005 Polycarbonate, Optical/Compact Disc Grade  (discontinued **)
Injection molding grade with exceptionally good flow, for optical storage media such as CD.Information provided by Bayer.As of 1 September 2015, Bayer MaterialScience was separated from Bayer AG and..
Melt Temperature 321 - 335 °C
610 - 635 °F
Solvay Specialty Polymers Amodel® A-6135 HN Polyphthalamide (PPA), 35% Glass Fiber (Conditioned)
Amodel® A-6135 HN polyphthalamide (PPA) is a 35% glass reinforced resin that is heat stabilized, lubricated and hot-water moldable. Key properties of the resin are high heat resistance, high stre..
Melt Temperature 321 - 335 °C
610 - 635 °F
Solvay Specialty Polymers Amodel® A-6135 HN Polyphthalamide (PPA), 35% Glass Fiber (Dry)
Amodel® A-6135 HN polyphthalamide (PPA) is a 35% glass reinforced resin that is heat stabilized, lubricated and hot-water moldable. Key properties of the resin are high heat resistance, high stre..
Melt Temperature 321 - 335 °C
610 - 635 °F
Solvay Specialty Polymers Amodel® AT-6115 HS Polyphthalamide (PPA), 15% Glass Fiber (Conditioned)
Amodel® AT-6115 HS is a 15% glass-fiber reinforced, toughened grade of polyphthalamide (PPA) resin designed to possess more elongation than other 15% glass-fiber reinforced grades of Amodel resin..
Melt Temperature 321 - 335 °C
610 - 635 °F
Solvay Specialty Polymers Amodel® AT-6115 HS Polyphthalamide (PPA), 15% Glass Fiber (Dry)
Amodel® AT-6115 HS is a 15% glass-fiber reinforced, toughened grade of polyphthalamide (PPA) resin designed to possess more elongation than other 15% glass-fiber reinforced grades of Amodel resin..
Melt Temperature 321 - 335 °C
610 - 635 °F
Solvay Specialty Polymers Amodel® AT-6130 HS Polyphthalamide (PPA), 30% Glass Fiber (Conditioned)
Amodel® AT-6130 HS is a 30% glass-reinforced, toughened polyphthalamide (PPA) resin that has more elongation than other 30% glass-reinforced grades of Amodel® resin. This grade was developed f..
Melt Temperature 321 - 335 °C
610 - 635 °F
Solvay Specialty Polymers Amodel® AT-6130 HS Polyphthalamide (PPA), 30% Glass Fiber (Dry)
Amodel® AT-6130 HS is a 30% glass-reinforced, toughened polyphthalamide (PPA) resin that has more elongation than other 30% glass-reinforced grades of Amodel® resin. This grade was developed f..
Melt Temperature 310 - 335 °C
590 - 635 °F
LATI LARAMID CE/60 60% Mineral Filled Polyphthalamide (PPA) Based Compound  (Unverified Data**)
Laramid compounds are based on a unique semi-crystalline engineering polymer (polyphthalamide) offering improved performance compared to traditional engineering thermoplastics at a lower cost than s..
Melt Temperature 321 - 335 °C
610 - 635 °F
Solvay Specialty Polymers Amodel® A-6135 HN Polyphthalamide (PPA)  (Unverified Data**)
Amodel A-6135 HN polyphthalamide (PPA) is a 35% glass reinforced resin that is heat stabilized, lubricated and hot-water moldable. Key properties of the resin are high heat resistance, high strength..
Melt Temperature 321 - 335 °C
610 - 635 °F
Solvay Specialty Polymers Amodel® AT-6130 HS Polyphthalamide (PPA)  (Unverified Data**)
Amodel AT-6130 HS is a 30% glass-reinforced, toughened polyphthalamide (PPA) resin that has more elongation than other 30% glass-reinforced grades of Amodel resin. This grade was developed for autom..
Melt Temperature 320 - 335 °C
608 - 635 °F
Solvay Specialty Polymers Amodel® A-6135 NL Polyphthalamide (PPA), 35% Glass Fiber Reinforcement  (discontin
Amodel A-6135 NL polyphthalamide (PPA), a 35% glass reinforced, high-glow, non-lubricated, hot-water moldable resin specially designed for laser welding. The black version is a laser absorber, and t..
Melt Temperature 310 - 335 °C
590 - 635 °F
LATI LARAMID G/30 30% Glass Filled Polyphthalamide (PPA) Based Compound  (Unverified Data**)
Laramid compounds are based on a unique semi-crystalline engineering polymer (polyphthalamide) offering improved performance compared to traditional engineering thermoplastics at a lower cost than s..
Melt Temperature 310 - 335 °C
590 - 635 °F
LATI LARAMID G/35 35% Glass Filled Polyphthalamide (PPA) Based Compound  (Unverified Data**)
Laramid compounds are based on a unique semi-crystalline engineering polymer (polyphthalamide) offering improved performance compared to traditional engineering thermoplastics at a lower cost than s..
Melt Temperature 310 - 335 °C
590 - 635 °F
LATI LARAMID G/45 45% Glass Filled Polyphthalamide (PPA) Based Compound  (Unverified Data**)
Laramid compounds are based on a unique semi-crystalline engineering polymer (polyphthalamide) offering improved performance compared to traditional engineering thermoplastics at a lower cost than s..
Melt Temperature 310 - 335 °C
590 - 635 °F
LATI LARAMID G/50 50% Glass Filled Polyphthalamide (PPA) Based Compound  (Unverified Data**)
Laramid compounds are based on a unique semi-crystalline engineering polymer (polyphthalamide) offering improved performance compared to traditional engineering thermoplastics at a lower cost than s..