Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Solvay Specialty Polymers Amodel® AS-4133 HS Polyphthalamide (PPA), 33% Glass Fiber (Conditioned)

Category Polymer , Thermoplastic , Polyphthalamide (PPA) , Polyphthalamide (PPA), 30% Glass Fiber Reinforced
Manufacturer Solvay Specialty Polymers
Trade Name Amodel®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Solvay Specialty Polymers Amodel® AS-4133 HS Polyphthalamide (PPA), 33% Glass Fiber (Conditioned).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Amodel® AS-4133 HS is a 33% glass reinforced, lubricated, heat stabilized grade of polyphthalamide (PPA) that offers fast cycle times and moldability in hot water molds. Testing conducted on samples dry as molded and samples conditioned to 50% relative humidity in accordance with ISO-1110, Accelerated Method. Typical applications include electrical and electronic components especially for automotive systems.Features: Fast Molding Cycle; Good Chemical Resistance; Good Creep Resistance; Good Dimensional Stability; Good Stiffness; Heat Stabilized; High Heat Resistance; High Strength; Hot Water Moldability; Laser Weldable; Low Moisture Absorption; LubricatedUses: Automotive Applications; Automotive Electronics; Automotive Under the Hood; Cell Phones; Connectors; Electrical/Electronic Applications; General Purpose; Industrial Applications; Industrial Parts; Lawn and Garden Equipment; Machine/Mechanical Parts; Metal Replacement; Thick-walled Parts; Valves/Valve PartsInjection Molding Notes: Amodel® compounds are shipped in moisture-resistant packages at moisture levels according to specifications. Sealed, undamaged bags should be preferably stored in a dry room at a maximum temperature of 50°C (122°F) and should be protected from possible damage. If only a portion of a package is used, the remaining material should be transferred into a sealable container. It is recommended that Amodel® resins be dried prior to molding.Automotive Specifications ASTM D4000 PA102 G35 Color: BK324 Black; ASTM D4000 PA102 G35 Color: NT Natural; ASTM D4000 PPA0121 G34 GB145 KD170 KN100 PN060 YI285 Color: BK324 Black; ASTM D4000 PPA0121 G34 GB145 KD170 KN100 PN060 YI285 Color: NT Natural; ASTM D6779 PA102G35; BOSCH N28 BN05-OX2 BN0515-GF35-3Anf01AM Color: NT Natural; BOSCH N28 BN05-OX2 BN0515-GF35-3Asw01AM Color: BK324 Black; CHRYSLER MS-DB-478 Type A CPN3598 Color: BK Black; CHRYSLER MS-DB-478 Type A CPN3972 Color: Natural; DELPHI M-2396 Color: BK324 Black; DELPHI M-2396 M2396001 Color: NT Natural; DELPHI M-2396 M2396002 Color: BK-324 Black; DELPHI M-2396 M239600x Color: BU474 Blue; DELPHI M-53291 Color: BU474 Blue; DELPHI M-53293 Color: BK324 Black; DELPHI M-53293 Color: NT Natural; DELPHI M-6081 Color: NT Natural; DELPHI M-6083 Color: BK324 Black; GM GMP.PPA.002 Color: BK324 Black; GM GMP.PPA.002 Color: NT Natural; GM GMW16357P-PPA-GF35 Color: Black; GM GMW16357P-PPA-GF35 Color: Natural; ISO 1874 PA6T/66, MH, 12-120, GF33 Color: BK324 Black; ISO 1874 PA6T/66, MH, 12-120, GF33 Color: NT Natural; TORRINGTON T-456 Color: BK324 Black; TRW S-13972700 Color: BK324 Black; TRW S-13972700 Color: NT Natural; TYCO 100-1392 Color: BK324 Black; TYCO 100-1392 Color: NT Natural; YAZAKI YPES-25-02-306 Color: BK324 Black; YAZAKI YPES-25-02-306 Color: NT NaturalInformation provided by Solvay Specialty Polymers.
Physical Properties Metric English Comments
Density 1.45 g/cc
0.0524 lb/in³
Dry; ISO 1183
Filler Content 33 %
33 %
Glass Fiber
Linear Mold Shrinkage, Flow 0.0050 cm/cm
0.0050 in/in
Dry
Linear Mold Shrinkage, Transverse 0.010 cm/cm
0.010 in/in
Dry; ASTM D955
Mechanical Properties Metric English Comments
Tensile Strength 172 MPa
24900 psi
ASTM D638
Elongation at Break 2.2 %
2.2 %
ASTM D638
Tensile Modulus 11.7 GPa
1700 ksi
ASTM D638
Flexural Strength 241 MPa
35000 psi
ASTM D790
Flexural Modulus 11.0 GPa
1600 ksi
ASTM D790
Compressive Strength 172 MPa
24900 psi
ASTM D695
Shear Strength 75.8 MPa
11000 psi
ASTM D732
Izod Impact, Notched 0.690 J/cm
1.29 ft-lb/in
ASTM D256
Electrical Properties Metric English Comments
Volume Resistivity 5.00e+14 ohm-cm
5.00e+14 ohm-cm
ASTM D257
Dielectric Constant 3.4

@Frequency 1.00e+6 Hz
3.4

@Frequency 1.00e+6 Hz
ASTM D150
4.3

@Frequency 60.0 Hz
4.3

@Frequency 60.0 Hz
ASTM D150
Dielectric Strength 20.0 kV/mm

@Thickness 1.60 mm
508 kV/in

@Thickness 0.0630 in
ASTM D149
Dissipation Factor 0.019

@Frequency 1.00e+6 Hz
0.019

@Frequency 1.00e+6 Hz
ASTM D150
0.020

@Frequency 60.0 Hz
0.020

@Frequency 60.0 Hz
ASTM D150
Comparative Tracking Index 600 V
600 V
UL 746
High Voltage Arc-Tracking Rate, HVTR 18.0 mm/min
0.709 in/min
UL 746
Processing Properties Metric English Comments
Rear Barrel Temperature 318 - 324 °C
604 - 615 °F
Front Barrel Temperature 327 - 332 °C
621 - 630 °F
Melt Temperature 329 - 343 °C
624 - 649 °F
Mold Temperature 65.6 - 93.3 °C
150 - 200 °F
Drying Temperature 120 °C

@Time 14400 sec
248 °F

@Time 4.00 hour
Moisture Content <= 0.045 %
<= 0.045 %
Descriptive Properties Value Comments
Additive Heat Stabilizer
Lubricant
Mold Release
Availability Africa & Middle East
Asia Pacific
Europe
Latin America
North America
Color Black; Natural
Form Pellets
Processing Technique Water-Heated Mold Injection Molding
RoHS Compliance RoHS Compliant
Users viewing this material also viewed the following: