Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Shear Strength | 75.8 MPa @Temperature 23.9 °C |
11000 psi @Temperature 75.0 °F |
Short Beam; Dry; ASTM D2344 |
Park Electrochemical Nelcote® V-376 Cyanate Ester Epoxy Prepregs, 4581 Quartz Reinforced Nelcote® V-376 is a Cyanate Ester matrix providing excellent electrical and mechanical properties for harsh aircraft, shipboard, and undersea applications for Radomes, Antenna, and Reflectors. Simp.. |
|||
Shear Strength | 75.8 MPa | 11000 psi | ASTM D732 |
Quadrant EPP Nylatron® MC® 901 Blue, Heat Stabilized, Type 6 (ASTM Product Data Sheet) Data provided by Quadrant Engineering Plastic ProductsBroadest size range availabilityGood mechanical and electrical propertiesIdeal balance of strength and toughnessCast as finished parts and near .. |
|||
Shear Strength | 76.0 MPa | 11000 psi | ASTM D732 |
Chevron Phillips Ryton® R10 5002C PPS Polyphenylene Sulfide
(discontinued **) Ryton® PPS is used in many electronic and automotive applications because of its high strength, favorable electrical properties, and high temperature stability.Data provided by the manufacturer.Sol.. |
|||
Shear Strength | 75.8 - 108 MPa | 11000 - 15700 psi | Average value: 91.3 MPa Grade Count:8 |
Overview of materials for Polyphthalamide (PPA), 50% Glass Fiber Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Polyphthalamide, 50% Glass Fiber Reinforced". Each property range of values reported is minimum and maxi.. |
|||
Shear Strength | 76.0 - 79.0 MPa | 11000 - 11500 psi | Average value: 77.0 MPa Grade Count:3 |
Overview of materials for Nylon 66, Glass Fiber/PTFE Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Glass Fiber/PTFE Filled". Each property range of values reported is minimum and maximum values.. |
|||
Shear Strength | 75.8 MPa @Thickness 15.7 mm |
11000 psi @Thickness 0.620 in |
ASTM D732 |
Industrial Laminates/Norplex NP680 Paper Base Laminate Description: Hot punching grade with electrical properties between NP611 to NP631.Thickness Tested: 0.062", 0.125" & 0.500" |
|||
Shear Strength | 75.8 MPa @Thickness 15.7 mm |
11000 psi @Thickness 0.620 in |
ASTM D732 |
Industrial Laminates/Norplex NP664 Paper Base Laminate Description: Low cost room temperature punching grade with mechanical and electrical properties similar to NP612. This version is made with pigment cover plies on the surface.Thickness Tested: 0.062.. |
|||
Shear Strength | 75.8 MPa | 11000 psi | ASTM D732 |
Solvay Specialty Polymers Amodel® A-4133 HH Polyphthalamide (PPA), 33% Glass Fiber (Conditioned) Amodel® A-4133 HH is a 33% glass fiber reinforced heat stabilized grade of polyphthalamide (PPA) that has been designed to provide outstanding property retention to thermal oxidative degradation .. |
|||
Shear Strength | 75.8 MPa | 11000 psi | ASTM D732 |
Solvay Specialty Polymers Amodel® A-4145 HH Polyphthalamide (PPA), 45% Glass Fiber (Conditioned) Amodel® A-4145 HH is a 45% glass fiber reinforced heat stabilized grade of polyphthalamide (PPA) that has been designed to provide outstanding property retention to thermal oxidative degradation .. |
|||
Shear Strength | 75.8 MPa | 11000 psi | ASTM D732 |
Solvay Specialty Polymers Amodel® AS-4133 HS Polyphthalamide (PPA), 33% Glass Fiber (Conditioned) Amodel® AS-4133 HS is a 33% glass reinforced, lubricated, heat stabilized grade of polyphthalamide (PPA) that offers fast cycle times and moldability in hot water molds. Testing conducted on samp.. |
|||
Shear Strength | 75.8 MPa | 11000 psi | ASTM D732 |
Solvay Specialty Polymers Amodel® AS-4133 L Polyphthalamide (PPA), 33% Glass Fiber (Conditioned) Amodel® AS-4133 L polyphthalamide (PPA) a 33% glass reinforced, lubricated, structural grade of polyphthalamide (PPA) that offers fast cycle times and is hot water moldable. Typical applications .. |
|||
Shear Strength | 75.8 MPa | 11000 psi | ASTM D732 |
Solvay Specialty Polymers Amodel® AS-4145 HS Polyphthalamide (PPA), 45% Glass Fiber (Conditioned) Amodel® AS-4145 HS polyphthalamide (PPA) is a 45% glass reinforced resin that is hot-water moldable. Key properties include high heat resistance, high strength and stiffness over a broad tempera.. |
|||
Shear Strength | 76.0 MPa | 11000 psi | as molded |
Sumitomo Bakelite Durez® 22257 Phenolic, Compression Grade Durez 22257 Black Phenolic is a two-stage, asbestos-free, medium impact molding material. It is designed for appliance and electrical applications where additional mechanical strength is required. .. |
|||
Shear Strength | 76.0 MPa | 11000 psi | as molded |
Sumitomo Bakelite Durez® 22257 Phenolic, Injection Grade Durez 22257 Black Phenolic is a two-stage, asbestos-free, medium impact molding material. It is designed for appliance and electrical applications where additional mechanical strength is required. .. |
|||
Shear Strength | 76.0 MPa @Temperature 22.0 °C |
11000 psi @Temperature 71.6 °F |
0° |
Hexcel® HexPly® 954-2A Curing Cyanate Resin, M55J Fiber Information provided by HexCel |
|||
Shear Strength | 76.0 MPa | 11000 psi | IL; pr EN 2563 |
Hexcel® HexPly® 920CX-FM40J-6-42% 125°C Curing Epoxy Matrix High modulus carbon, Unidirectional, 165 g/m2Information provided by HexCel |
|||
Shear Strength | 76.0 MPa @Temperature 23.0 °C |
11000 psi @Temperature 73.4 °F |
DAM; ASTM D732 |
DuPont Performance Polymers Zytel® 77G33HS1L NC010 Nylon 612 Zytel® 77G33HS1L NC010 is a 33% glass fiber reinforced, heat stabilized polyamide 612 resin for injection molding.Information provided by DuPont Performance Polymers |
|||
Shear Strength | 76.0 MPa | 11000 psi | ASTM D732 |
Ascend Performance Materials VYDYNE® R513 Nylon, 13% Glass Reinforced Typical property data. VYDYNE is a registered trademark of Solutia Inc. |
|||
Shear Strength | 75.8 - 105 MPa | 11000 - 15300 psi | Average value: 92.4 MPa Grade Count:7 |
Overview of materials for Polyetheretherketone, Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Polyetheretherketone, Glass Fiber Filled". Each property range of values reported is minimum and maximum.. |
|||
Shear Strength | 75.8 MPa | 11000 psi | ASTM D732 |
Quadrant EPP Nylatron® MC® 907 Natural Nylon, Monocast® FDA Compliant, Unfilled Type 6 (ASTM Product Data Sheet) |
|||
Shear Strength | 75.8 MPa | 11000 psi | ASTM D732 |
Quadrant EPP Quadrant Nylon 105 Black |
|||
Shear Strength | 76.0 MPa | 11000 psi | ASTM D732 |
Chevron Phillips Ryton® R10 7006A PPS Polyphenylene Sulfide
(discontinued **) Ryton® PPS is used in many electronic and automotive applications because of its high strength, favorable electrical properties, and high temperature stability.Data provided by the manufacturer.Sol.. |
|||
Shear Strength | 75.8 MPa | 11000 psi | Conditioned; ASTM D732 |
Solvay Specialty Polymers Amodel® AS-4133 L Polyphthalamide (PPA)
(Unverified Data**) Amodel AS-4133 L polyphthalamide (PPA) a 33% glass reinforced, lubricated, structural grade of polyphthalamide (PPA) that offers fast cycle times and is hot water moldable. Typical applications incl.. |
|||
Shear Strength | 75.8 MPa | 11000 psi | ASTM D732 |
Quadrant EPP Ketron® CM CA30 PEEK Polyetheretherketone, 30% carbon fiber reinforced, compression molded (ASTM Product Data Sheet) Data provided by Quadrant Engineering Plastic Products Excellent chemical resistance Very low moisture absorption Inherently good wear and abrasion resistance Unaffected by continuous exposure to ho.. |
|||
Shear Strength | 75.8 MPa | 11000 psi | Conditioned; ASTM D732 |
Solvay Specialty Polymers Amodel® AS-4145 HS Polyphthalamide (PPA)
(Unverified Data**) Amodel AS-4145 HS polyphthalamide (PPA) is a 45% glass reinforced resin that is hot-water moldable. Key properties include high heat resistance, high strength and stiffness over a broad temperature.. |
|||
Shear Strength | 75.8 MPa | 11000 psi | ASTM D732 |
Solvay Specialty Polymers Amodel® AS-4133 HN Polyphthalamide (PPA), Conditioned
(discontinued **) Availability: Asia Pacific; Europe; North AmericaInformation provide by Solvay Specialty Polymers |