Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Melt Temperature = 329 °C Product List

Processing Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Processing Properties Metric English Comments
Melt Temperature 329 - 343 °C
625 - 650 °F
RTP Company RTP 4001 A FR (Hot Water Moldable) Polyphthalamide (PPA), Glass Fiber - Flame Retardant
Melt Temperature 329 - 343 °C
625 - 650 °F
RTP Company RTP 4002 A (Hot Water Moldable) Polyphthalamide (PPA), Glass Fiber
Melt Temperature 329 - 343 °C
625 - 650 °F
RTP Company RTP 4002 A FR (Hot Water Moldable) Polyphthalamide (PPA), Glass Fiber - Flame Retardant
Melt Temperature 329 - 343 °C
625 - 650 °F
RTP Company RTP 4003 A (Hot Water Moldable) Polyphthalamide (PPA), Glass Fiber
Melt Temperature 329 - 343 °C
625 - 650 °F
RTP Company RTP 4003 A FR (Hot Water Moldable) Polyphthalamide (PPA), Glass Fiber - Flame Retardant
Melt Temperature 329 - 343 °C
624 - 649 °F
Solvay Specialty Polymers Amodel® A-1130 FW Polyphthalamide (PPA)  (Unverified Data**)
Amodel A-1130 FW is a 30% glass-fiber reinforced polyphthalamide (PPA) grade containing a solid lubricant. This resin was designed for moderate-pressure, low-velocity friction and wear applications...
Melt Temperature 329 - 343 °C
625 - 650 °F
RTP Company RTP 4007 A (Hot Water Moldable) Polyphthalamide (PPA), Glass Fiber
Melt Temperature 329 - 343 °C
625 - 650 °F
RTP Company RTP 4007 A FR (Hot Water Moldable) Polyphthalamide (PPA), Glass Fiber - Flame Retardant
Melt Temperature 329 - 343 °C
624 - 649 °F
Solvay Specialty Polymers Amodel® A-4122 LS WH678 Polyphthalamide (PPA)  (Unverified Data**)
Amodel A-4122 LS is a 22% glass fiber reinforced, light-stabilized, high-reflectivity white grade of Amodel polyphthalamide (PPA). It is designed to provide high crystallinity when molded in water-c..
Melt Temperature 329 - 343 °C
624 - 649 °F
Solvay Specialty Polymers Amodel® A-4122 NL WH 905 Polyphthalamide (PPA)  (Unverified Data**)
Amodel A-4122 NL resin is a 22% glass reinforced, high-reflectivity white grade of polyphthalamide (PPA), designed to provide high crystallinity when molded in water-cooled molds. This material exhi..
Melt Temperature 329 - 343 °C
624 - 649 °F
Solvay Specialty Polymers Amodel® A-4160 HSL Polyphthalamide (PPA)  (Unverified Data**)
Amodel A-4160 HSL resin is a 60% glass reinforced, heat stabilized polyphthalamide (PPA) which exhibits high modulus at elevated temperatures, a high heat deflection temperature and exceptional cree..
Melt Temperature 329 - 343 °C
625 - 650 °F
RTP Company RTP 4008 A (Hot Water Moldable) Polyphthalamide (PPA), Glass Fiber
Melt Temperature 329 - 343 °C
625 - 650 °F
RTP Company RTP 4008 A FR (Hot Water Moldable) Polyphthalamide (PPA), Glass Fiber - Flame Retardant
Melt Temperature 329 - 343 °C
625 - 650 °F
RTP Company RTP 4009 A MS (Hot Water Moldable) Polyphthalamide (PPA), Glass Fiber Reinforced - Molybdenum Disulfide Lubricated
Melt Temperature 329 - 343 °C
625 - 650 °F
RTP Company RTP 4011 A (Hot Water Moldable) Polyphthalamide (PPA), Glass Fiber
Melt Temperature 329 - 343 °C
625 - 650 °F
RTP Company RTP 4085 A (Hot Water Moldable) Polyphthalamide (PPA), Carbon Fiber
Melt Temperature 329 - 343 °C
625 - 650 °F
RTP Company RTP 4087 A FR (Hot Water Moldable) Polyphthalamide (PPA), Carbon Fiber - Flame Retardant
Melt Temperature 329 - 385 °C
624 - 725 °F
Solvay Specialty Polymers Udel® P-1710 Polysulfone (PSU)  (Unverified Data**)
Udel P-1710 polysulfone (PSU) is a tough, rigid, high-strength thermoplastic that is suitable for continuous use up to 300°F (149°C). The resin is resistant to oxidation and hydrolysis and withsta..
Melt Temperature 329 - 385 °C
624 - 725 °F
Solvay Specialty Polymers Udel® P-1720 Polysulfone (PSU)  (discontinued **)
Udel P-1720 is a flame-retardant grade of polysulfone (PSU) that has a UL94 rating of V-0 at a thickness of 1 mm (0.039"). In general, polysulfone is a tough, rigid, high-strength thermoplastic that..
Melt Temperature 329 - 385 °C
624 - 725 °F
Solvay Specialty Polymers Udel® P-1750 MR Polysulfone (PSU)  (Unverified Data**)
Udel P-1750 MR is a lower color grade of polysulfone that contains a mold release which aids part ejection when parts with low draft are injection molded. Polysulfones have long been known for trans..
Melt Temperature 329 - 385 °C
624 - 725 °F
Solvay Specialty Polymers Udel® P-3703 Polysulfone (PSU)  (Unverified Data**)
Udel P-3703 is a high-flow grade of polysulfone intended for injection molding applications with thin walls or long flow lengths. This grade has higher flow than Udel P-1700 and a slightly greater t..
Melt Temperature 329 - 343 °C
624 - 649 °F
Solvay Specialty Polymers Amodel® A-4133 HH Polyphthalamide (PPA), 33% Glass Fiber (Dry)
Amodel® A-4133 HH is a 33% glass fiber reinforced heat stabilized grade of polyphthalamide (PPA) that has been designed to provide outstanding property retention to thermal oxidative degradation ..
Melt Temperature 329 - 343 °C
624 - 649 °F
Solvay Specialty Polymers Amodel® A-4160 HSL Polyphthalamide (PPA), 60% Glass Fiber
Amodel® A-4160 HSL resin is a 60% glass reinforced, heat stabilized polyphthalamide (PPA) which exhibits high modulus at elevated temperatures, a high heat deflection temperature and exceptional ..
Melt Temperature 329 - 343 °C
624 - 649 °F
Solvay Specialty Polymers Amodel® AS-4133 HS Polyphthalamide (PPA), 33% Glass Fiber (Dry)
Amodel® AS-4133 HS is a 33% glass reinforced, lubricated, heat stabilized grade of polyphthalamide (PPA) that offers fast cycle times and moldability in hot water molds. Testing conducted on samp..
Melt Temperature 329 - 343 °C
624 - 649 °F
Solvay Specialty Polymers Amodel® AS-4133 L Polyphthalamide (PPA), 33% Glass Fiber (Conditioned)
Amodel® AS-4133 L polyphthalamide (PPA) a 33% glass reinforced, lubricated, structural grade of polyphthalamide (PPA) that offers fast cycle times and is hot water moldable. Typical applications ..
Melt Temperature 329 - 343 °C
624 - 649 °F
Solvay Specialty Polymers Amodel® AS-4145 HS Polyphthalamide (PPA), 45% Glass Fiber (Conditioned)
Amodel® AS-4145 HS polyphthalamide (PPA) is a 45% glass reinforced resin that is hot-water moldable. Key properties include high heat resistance, high strength and stiffness over a broad tempera..
Melt Temperature 329 - 385 °C
624 - 725 °F
Solvay Specialty Polymers Udel® P-3700 HC Polysulfone (PSU)
Udel® P-3700 HC is a high-clarity grade of polysulfone (PSU) that is nearly water-white in color. This grade was designed to eliminate the yellow cast and provide design flexibility and improved ..
Melt Temperature 329 - 385 °C
624 - 725 °F
Solvay Specialty Polymers Udel® P-3703 Polysulfone (PSU)
Udel® P-3703 is a high-flow grade of polysulfone intended for injection molding applications with thin walls or long flow lengths. This grade has higher flow than Udel® P-1700 and a slightly g..
Melt Temperature 329 - 385 °C
624 - 725 °F
Solvay Specialty Polymers Udel® P-1700 Polysulfone (PSU)
Udel® P-1700 polysulfone (PSU) is a tough, rigid, high-strength thermoplastics suitable for continuous use up to 300°F (149°C). It is resistant to oxidation and hydrolysis and withstand pro..
Melt Temperature 329 - 341 °C
624 - 646 °F
Solvay Specialty Polymers Amodel® AFA-4133 V0 Z Polyphthalamide (PPA), Dry  (discontinued **)
Amodel AFA-4133 V0 Z is a 33% glass-fiber reinforced, flame retardant grade of polyphthalamide (PPA) resin specifically formulated for connector applications requiring compatibility with both infrar..
Copyright © lookpolymers.com All Rights Reserved