Tensile Modulus 11.7 GPa
1700 ksi
ASTM D-638
Glastic 1120 Corrosion-Resistant Panels
Glastic® Corrosion-Resistant Panels are ideal for applications where resistance to both flame, and the splash or spill of laboratory chemicals is important. Glastic® Grade 1120 is an asbestos..
Tensile Modulus 11.7 GPa
1700 ksi
ASTM D-638
Glastic 1125 Corrosion-Resistant Panels
Glastic® Corrosion-Resistant Panels are ideal for applications where resistance to both flame, and the splash or spill of laboratory chemicals is important. Glastic® Grade 1125 is asbestos-fr..
Tensile Modulus 11.7 GPa
1700 ksi
ASTM D-638
Glastic SG-200 Industrial Lift Magnet
Glastic Grade SG-200 high-strength and high-temperature laminates offer temperature ratings of up to 210°C. SG-200 is ideal for a wide variety of product applications requiring high-temperature ..
Tensile Modulus 11.7 GPa
1700 ksi
ISO 527 Type 1A
Solvay TECHNYL® A 60 G1 V30 PA66, 30% glass fiber, DRY
Description: Flame retardant Polyamide PA66 reinforced with 30% of glass fiber, for injection molding.Available in: Asia Pacific, Europe, Latin America and North AmericaProduct Applications: This R..
Tensile Modulus 11.72 GPa
1700 ksi
5 mm/min; ASTM D 638
SABIC Innovative Plastics Ultem 3451 PEI (Asia Pacific)
45% Glass fiber and mineral filled, standard flow Polyetherimide (Tg 217C) with enhanced dimensional stability. ECO Conforming.This data was supplied by SABIC-IP for the Asia Pacific region.
Tensile Modulus 11.7 GPa
1700 ksi
ASTM D638
Solvay Specialty Polymers Amodel® AS-4133 HS Polyphthalamide (PPA), 33% Glass Fiber (Conditioned)
Amodel® AS-4133 HS is a 33% glass reinforced, lubricated, heat stabilized grade of polyphthalamide (PPA) that offers fast cycle times and moldability in hot water molds. Testing conducted on samp..
Tensile Modulus 11.7 GPa
1700 ksi
ASTM D638
Solvay Specialty Polymers Amodel® AS-4133 L Polyphthalamide (PPA), 33% Glass Fiber (Dry)
Amodel® AS-4133 L polyphthalamide (PPA) a 33% glass reinforced, lubricated, structural grade of polyphthalamide (PPA) that offers fast cycle times and is hot water moldable. Typical applications ..
Tensile Modulus 11.72 GPa
1700 ksi
50 mm/min; ASTM D638
SABIC Innovative Plastics LNP STAT-KON ZE0039 PPO
LNP* STAT-KON* ZE0039 is a compound based on PPO resin containing 15% Carbon Fiber. Added features of this grade includes: Flame Retardant, Electrically Conductive.
Tensile Modulus 11.72 GPa
1700 ksi
5 mm/min; ASTM D638
SABIC Innovative Plastics LNP THERMOCOMP D451 PC (Asia Pacific)
LNP* Thermocomp* D451 (or EXTC8141) is a compound based on Polycarbonate resin containing Glass Fiber, Flame Retardant. Added features of this material include: High modulus, good flatness, good duc..
Tensile Modulus 11.72 GPa
1700 ksi
50 mm/min; ASTM D638
SABIC Innovative Plastics LNP THERMOCOMP DE004ERP PC (Asia Pacific)
LNP* Thermocomp* DE004ERP is a compound based on Polycarbonate resin containing Carbon Fiber. Added features of this material include: Electrically Conductive, Easy Molding, Mold Release.
Tensile Modulus 11.72 GPa
1700 ksi
5 mm/min; ASTM D638
SABIC Innovative Plastics ULTEM HU2410 PEI
40% Glass fiber filled, enhanced flow Polyetherimide (Tg 217C). ECO Conforming. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO 10993 or USP..
Tensile Modulus 11.7 GPa
1700 ksi
DAM; ISO 527-1/-2
DuPont Performance Polymers Zytel® 80G43HS1L BK104 Nylon 66  (Unverified Data**)
43% Glass Reinforced Toughened Heat Stabilized Polyamide 66 Zytel 80G43HS1L BK104 is a 43% glass fiber reinforced heat stabilized black polyamide 66 resin with superior impact resistance.Information..
Tensile Modulus 11.7 GPa
1700 ksi
DAM; ISO 527-1/-2
DuPont Performance Polymers Zytel® HTN FG52G35HSL BK011 Polyphthalamide (PPA)  (Unverified Data**)
35% Glass Reinforced PPA High Performance Polyamide Zytel HTNFG52G35HSL BK011 is a 35% glass reinforced lubricated heat stabilized high performance polyamide resin developed for consideration into a..
Tensile Modulus 11.7 GPa
1700 ksi
ASTM D638
Applied Composites 8052 Polyester SMC
Industry Application: RecreationProduct Application: Marine ProductsDistinct Features: High Strength, ResilientInformation provided by Applied Composites Corporation.
Tensile Modulus 11.7 GPa
1700 ksi
ASTM D638
Solvay Specialty Polymers Amodel® AS-4133 L Polyphthalamide (PPA)  (Unverified Data**)
Amodel AS-4133 L polyphthalamide (PPA) a 33% glass reinforced, lubricated, structural grade of polyphthalamide (PPA) that offers fast cycle times and is hot water moldable. Typical applications incl..
Tensile Modulus 11.7 GPa
1700 ksi
ASTM D638
Solvay Specialty Polymers Amodel® AS-4133 HN Polyphthalamide (PPA), Conditioned  (discontinued **)