H.C. Starck Baymetec® Tantalum n-Butoxide

Category Ceramic , Oxide
Manufacturer H.C. Starck
Trade Name Baymetec®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF H.C. Starck Baymetec® Tantalum n-Butoxide.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Physical Properties Metric English Comments
Density 1.30 g/cc
0.0470 lb/in³
Thermal Properties Metric English Comments
Melting Point <= 21.0 °C
<= 69.8 °F
Boiling Point 195 °C
383 °F
.5 hPa
Descriptive Properties Value Comments
Color none