ATI Allvac® VascoJet® 1000 Specialty Steel, Heat Treatment: 1010°C (1850°F) Q+T

Category Metal , Ferrous Metal , Tool Steel
Manufacturer ATI Allvac
Trade Name VascoJet®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF ATI Allvac® VascoJet® 1000 Specialty Steel, Heat Treatment: 1010°C (1850°F) Q+T.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Data provided by Allvac.Applications: Landing gear components, springs, fasteners. Gears and shafts for helicopter applications.
Physical Properties Metric English Comments
Density 7.75 g/cc
0.280 lb/in³
Mechanical Properties Metric English Comments
Hardness, Brinell 422
422
Estimated from Rockwell C value for Brinell test with 3000 kg load/10 mm diameter ball
Hardness, Knoop 463
463
Estimated from Rockwell C value.
Hardness, Rockwell C 45
45
Hardness, Vickers 442
442
Estimated from Rockwell C value.
Tensile Strength, Ultimate 1524 MPa
221000 psi
Tensile Strength, Yield 1303 MPa

@Strain 0.200 %
189000 psi

@Strain 0.200 %
Elongation at Break 38 %
38 %
Reduction of Area 11 %
11 %
Component Elements Properties Metric English Comments
Carbon, C 0.40 %
0.40 %
Chromium, Cr 5.0 %
5.0 %
Iron, Fe 92 %
92 %
as balance
Manganese, Mn 0.30 %
0.30 %
Molybdenum, Mo 1.3 %
1.3 %
Silicon, Si 0.90 %
0.90 %
Vanadium, V 0.50 %
0.50 %