Material Notes:
Description: DEXFLEX® 880 is a thermoplastic olefinic elastomer (TPO) designed for automotive exterior applications that require a combination of stiffness, low-temperature impact, good processability, and excellent weatherability. Applications: Bumper fascias and other large components that must exhibit durable paintability in exterior body colors. Information provided by Solvay Engineered Polymers.LyondellBasell acquired Solvay Engineered Polymers in 2008. This grade is not part of the current LyondellBasell product line.
Physical Properties Metric English Comments
Specific Gravity 0.900 g/cc
0.900 g/cc
ASTM D792
Linear Mold Shrinkage 0.0080 - 0.011 cm/cm
0.0080 - 0.011 in/in
as molded; ASTM D995
0.012 - 0.015 cm/cm
0.012 - 0.015 in/in
after bake; ISO 294
Melt Flow 14 g/10 min
14 g/10 min
ISO 1133
Mechanical Properties Metric English Comments
Tensile Strength, Yield 15.0 MPa
2180 psi
2 in/min; ASTM D638
Flexural Modulus 0.552 GPa
80.1 ksi
I.B., TAN, 0.5 in/min; ASTM D790
Thermal Properties Metric English Comments
CTE, linear 108 µm/m-°C

@Temperature 20.0 °C
60.0 µin/in-°F

@Temperature 68.0 °F
modified; ASTM D696